Integrated fully-sealed liquid crystal screen and manufacturing process for same
A manufacturing process and fully-sealed technology, applied in optics, instruments, electrical digital data processing, etc., can solve the problems of easy moiré, dull defective products, and difficult defoaming due to differences in display screens, and achieve good solid-state fluidity Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] A manufacturing process for a fully sealed liquid crystal integrated screen, which uses solid ultraviolet flexible glue to bond sequentially arranged components to form a whole, and the components include a touch screen group 11, a support frame 13 and a glass rear cover 14; its process include:
[0035] 1) Paste a piece of solid ultraviolet flexible glue with a thickness of 50-100 μm between any two adjacent components, and the support frame 13 is embedded with a liquid crystal screen group 12 and an edge-lit backlight module 15;
[0036] 2) Degassing: Put the components attached with solid ultraviolet flexible glue into the autoclave for 10-50 minutes for degassing, control the pressure in the autoclave to 0.5kg-3kg, and the temperature to 30-40℃;
[0037] 3) Curing: Use a high-power UV lamp to irradiate the transparent glued body with strong light, so that the solid-state ultraviolet flexible glue can be cured and bonded to each component;
[0038] 4) Edge sealing: ...
Embodiment 2-3
[0042] Using the same preparation method as in Example 1, the difference is that the thickness, pressure and temperature in the pre-lamination and degassing steps listed in Table 1 are used to replace the corresponding values used in Example 1 to obtain different sizes of fully sealed LCD integrated screen.
[0043] Table 1
[0044]
[0045] In the embodiment, if the thickness of the solid ultraviolet flexible adhesive is less than 50 μm, the fluidity is not enough, and thickness difference is likely to occur. If the thickness is higher than 300 μm, the fluidity is too full and overflowing glue is likely to occur. If the temperature and pressure are lower than the limit value, the solid ultraviolet flexible adhesive will not be easily bonded to each component; during the defoaming process, the temperature is 30-65°C, the pressure is 0.5-10kg, and the defoaming time is 10-250 minutes. If the value is higher than the limit value, the The resin is easy to soften and cause...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com