A production method and bobbin paper technology, applied in the direction of adhesives, non-polymer adhesive additives, adhesive additives, etc., can solve the problems of slow sizing speed, poor stability and water resistance, depolymerization reaction, etc., to achieve Increased sizing speed, small amount of sizing, and strong adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Benefits of technology
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A bobbin paper glue, made of the following raw materials in parts by weight: 40 parts of cornstarch and potato starch in a weight ratio of 4:1, 6 parts of borax and boric acid in a weight ratio of 7:2, 0.8 parts of sodium hydroxide, 50 parts of water, 8 parts of vinyl acetate, 2 parts of filler.
[0023] A kind of above-mentioned preparation method of bobbin paper glue, comprises the following steps:
[0024] Put the aged starch into the reaction container, add water and stir for 10-15 minutes at a stirring speed of 80-160 rpm to a uniformly mixed starch liquid; configure sodium hydroxide with a concentration of 8-12%, and ultrasonically oscillate evenly Add the prepared starch liquid, add sodium hydroxide solution while stirring, and stir until the shape of the solution does not change; then add cross-linking agent, vinyl acetate, filler, and continue stirring for 20-30 minutes.
[0025] Wherein, the preparation method of the aged starch comprises the following steps:...
Embodiment 2
[0028] A bobbin paper glue, made of the following raw materials in parts by weight: 45 parts of cornstarch and potato starch in a weight ratio of 5:1, 7 parts of borax and boric acid in a weight ratio of 7:2, 0.9 parts of sodium hydroxide, 55 parts of water, 9 parts of vinyl acetate, 3 parts of silicate and light calcium carbonate with a ratio of 0.5:1.
[0029] A kind of above-mentioned preparation method of bobbin paper glue, comprises the following steps:
[0030] Put the aged starch into the reaction container, add water and stir for 12.5 minutes at a stirring speed of 120 rpm to a uniform starch liquid; configure sodium hydroxide with a concentration of 10%, and add the starch prepared above after ultrasonic oscillation solution, add sodium hydroxide solution while stirring, and stir until the shape of the solution does not change; then add crosslinking agent, vinyl acetate, filler, and continue stirring for 25 minutes.
[0031] Wherein, the preparation method of the des...
Embodiment 3
[0033] A bobbin paper glue, made of the following raw materials in parts by weight: a total of 50 parts of cornstarch and potato starch in a weight ratio of 6:1, 8 parts of borax and boric acid in a weight ratio of 7:1, and 1 part of sodium hydroxide , 60 parts of water, 10 parts of vinyl acetate, 4 parts of filler with a ratio of 0.5:1 silicate and light calcium carbonate.
[0034] A kind of above-mentioned preparation method of bobbin paper glue, comprises the following steps:
[0035] Put the aged starch into the reaction container, add water and stir for 15 minutes at a stirring speed of 160 rpm to a uniform starch liquid; configure sodium hydroxide with a concentration of 12%, and add the starch prepared above after ultrasonic oscillation solution, add sodium hydroxide solution while stirring, and stir until the shape of the solution does not change; then add cross-linking agent, vinyl acetate, filler, and continue stirring for 30 minutes.
[0036]Wherein, the preparatio...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com