An inspection method for chemically milled weight-reducing grooves of parts
A technology of weight-reducing grooves and parts, which is applied in the inspection field of part chemical milling weight-reducing grooves, can solve the problems of low precision, difficulty, and high price, and achieve the effects of improving inspection efficiency, improving inspection accuracy, and reducing inspection costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0022] The present invention will be described in further detail below, a kind of inspection method of part chemical milling weight-reducing groove, comprises the following steps:
[0023] A method for inspecting weight-reducing grooves by chemical milling of parts, comprising the following steps:
[0024] In the first step, in the three-dimensional model of part 1, make the largest projection plane P of part 1, project the outer contour line a of the part on the projection plane P along the normal direction of the projection plane P, and obtain the projection line of the outer contour line of the part a1; Project the edge line b of the milling weight-reducing groove of the part onto the projection plane P along the normal direction of the projection plane P, and obtain the projection line b1 of the edge line of the milling weight-reducing groove of the part. Such as figure 1 shown.
[0025] In the second step, on the steel plate with a thickness of 10 mm to 20 mm, the outer...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 