[0064] refer to Figure 1 to Figure 3 , a magnetic building block that can be folded and adsorbed arbitrarily according to the present invention, comprising no less than one unit member sheet forming the building block, characterized in that the unit member is provided with four creases 2 on the core layer 1 and closely connected with the The flexible amphoteric magnetic layer 3 outside the crease area on both sides of the outer side of the core layer, the thickness of the amphipathic magnetic layer is 0.7mm, the core layer 1 is an isosceles trapezoidal synthetic paper sheet with a thickness of 0.15mm, and the crease 2 2 parallel indentations are set on the edge, chamfers are set at both ends of the creases, the width of the creases is not less than 1.9mm, and the creases divide the core layer into 5 equilateral triangles that are closely arranged in staggered planes , the side length of the triangle is 48mm, and the area of the core layer is the sum of the areas of 5 equila...
Embodiment 2
[0079] refer to Figure 5 with Image 6 , the present invention is a foldable magnetic building block that can be adsorbed arbitrarily. This embodiment is the same as embodiment 1 except that the fabrication of the bisexual magnetic layer is different from embodiment 1 as follows.
[0080] The making of described bisexual magnetic layer magnetic layer is as follows:
[0081] Ingredients: Refer to Table 1 below.
[0082] Internal mixing: mix the anisotropic ferrite powder and soft magnetic powder according to the proportions in Table 1, respectively, using an internal mixer to mix the rubber, and the clinker is discharged after the mixing temperature reaches 120~150°C.
[0083] Open refining: use the open mixer to mix the mixed materials separately.
[0084] Refining and crushing: Refining the refined film into small balls with an internal mixer and crushing with a crusher.
[0085] Calendering: The crushed pellets are directly calendered using a calender to process anisotr...