Drought region chili planting soil improvement agent and preparation method thereof
A soil conditioner and pepper technology, which is applied to fertilizers made from biological waste, applications, organic fertilizers, etc., can solve the problems of unrealistic soil drought, unstable water retention performance, and unsuitable drip irrigation, etc., to improve soil adhesion. The effect of focusing force, capillary adsorption force, and critical surface tension increase
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A soil improver for pepper planting in arid areas, the components are as follows by weight: 15 parts of bentonite, 20 parts of kaolin, 15 parts of perlite, 5 parts of soybean cake, 15 parts of peat, 20 parts of manure, 20 parts of straw, and nanometer titanium dioxide Modified resin additive 25 parts.
[0026] Preferably, the manure is prepared by mixing cow manure, pig manure, sheep manure and chicken manure in a weight ratio of 1:1:1.5:2.
[0027] Preferably, the straw is prepared by mixing corn straw, wheat straw and soybean straw in a weight ratio of 1:1:1.5.
[0028] As preferably, the preparation method of wherein said nano-titanium dioxide modified resin additive is as follows:
[0029] 1) Take 17 parts of sucrose, add 32 parts of deionized water, stir the solution to form a clear and transparent solution, add 4 parts of polytetrafluoroethylene, mix and stir, place in a muffle furnace for heating, the heating temperature is 180 ° C, the heating time 4h;
[003...
Embodiment 2
[0039] A soil improver for pepper planting in arid areas, the components are as follows by weight: 17 parts of bentonite, 25 parts of kaolin, 20 parts of perlite, 10 parts of soybean cake, 17 parts of peat, 25 parts of manure, 25 parts of straw, and nanometer titanium dioxide 27 parts of modified resin additives.
[0040] Preferably, the manure is prepared by mixing cow manure, pig manure, sheep manure and chicken manure in a weight ratio of 1:1:1.5:2.
[0041] Preferably, the straw is prepared by mixing corn straw, wheat straw and soybean straw in a weight ratio of 1:1:1.5.
[0042] As preferably, the preparation method of wherein said nano-titanium dioxide modified resin additive is as follows:
[0043] 1) Take 20 parts of sucrose, add 35 parts of deionized water, stir the solution to form a clear and transparent solution, add 5 parts of polytetrafluoroethylene, mix and stir, place in a muffle furnace for heating, the heating temperature is 200 ° C, the heating time 4.5 ho...
Embodiment 3
[0053] A soil improver for capsicum planting in arid areas, the components are as follows by weight: 20 parts of bentonite, 30 parts of kaolin, 25 parts of perlite, 15 parts of soybean cake, 20 parts of peat, 30 parts of manure, 30 parts of straw, nano titanium dioxide 30 parts of modified resin additives.
[0054] Preferably, the manure is prepared by mixing cow manure, pig manure, sheep manure and chicken manure in a weight ratio of 1:1:1.5:2.
[0055] Preferably, the straw is prepared by mixing corn straw, wheat straw and soybean straw in a weight ratio of 1:1:1.5.
[0056] As preferably, the preparation method of wherein said nano-titanium dioxide modified resin additive is as follows:
[0057] 1) Take 26 parts of sucrose, add 45 parts of deionized water, stir the solution to form a clear and transparent solution, add 8 parts of polytetrafluoroethylene, mix and stir, place in a muffle furnace for heating, the heating temperature is 210 ° C, the heating time 5h;
[0058]...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com