Hydrated calcium silicate early strength agent and preparation method thereof

A technology of calcium silicate hydrate and early strength agent, which is applied in the direction of silicate, alkaline earth metal silicate, etc., can solve the problem of reducing the performance of calcium silicate hydrate, the particle size of calcium silicate hydrate is large, and cannot To adapt to high-speed development and other issues, to achieve the effect of shortening the coagulation time, high dispersion, and lowering the nucleation energy barrier

Active Publication Date: 2019-04-19
KZJ NEW MATERIALS GROUP CO LTD
View PDF8 Cites 20 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, the above-mentioned scheme is still insufficient in shortening the setting time of cement. The 1d compressive strength test is only 12.6MPa, which is still unable to adapt to the rapid development of the current construction industry.
[0004] Existing methods for preparing calcium silicate hydrate, such as the hydrothermal method, often need to use a reactor as a reaction vessel, and the reaction needs to be carried out under high temperature and high pressure conditions, and the energy consumption is also high; the precipitation method takes too long and the benefit is not high
[0005] In addition, the calcium silicate hydrate particles in the calcium silicate hydrate early strength agent prepared by the prior art are prone to uneven mixing and agglomeration, resulting in too large a particle size of the calcium silicate hydrate particles, poor dispersion, and reduced silicon hydrate. The performance effect of calcium acid

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Hydrated calcium silicate early strength agent and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0033] (1) Calcium liquid preparation: select papermaking waste lime mud as the calcium source, after further crushing, first raise the temperature to 150°C at a rate of 5°C / min, and keep the temperature constant for 30 minutes; then, heat up at 10°C / min The heating rate was raised to 600°C, and the temperature was kept constant for 1 hour; finally, the temperature was raised to 800°C at a heating rate of 5°C / min, and the temperature was kept constant for 2 hours; after natural cooling, the obtained product was sieved and washed 4 times with distilled water repeatedly. Soak in 0.5 mol / L nitric acid solution for 12 hours, filter out impurities; add distilled water to the filtrate to adjust the solubility of calcium ions to 3 mol / L, age for 10 hours, and use it as a calcium solution for later use.

[0034] (2) Preparation of silicon liquid: select tetraethylorthosilicate as the silicon source, add distilled water, adjust the solubility of silicon ions to 1 mol / L, and use it as th...

Embodiment 2

[0038] This example is basically the same as the preparation method of a calcium silicate hydrate accelerator described in Example 1, except that the reaction temperature in step (4) is increased from 25°C to 50°C.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
compressive strengthaaaaaaaaaa
Login to view more

Abstract

The invention relates to the technical field of building materials, in particular to a hydrated calcium silicate early strength agent and a preparation method thereof. The preparation method of the hydrated calcium silicate early strength agent comprises the following preparation steps of: 1) preparing calcium solution; 2) preparing silicon liquid by taking silicate ester as a silicon source; 3) synthesis of hydrated calcium silicate: placing dispersant solution prepared by compounding polyoxyethylene (5) nonyl phenyl ether and cyclohexane into a shearing and stirring mixing device, keeping stirring at room temperature, adding prepared calcium solution and silicon solution, adjusting the pH value of mixed solution by using alkaline solution, stirring at constant temperature to obtain whitehydrated calcium silicate gel; centrifugally washing obtained white hydrated calcium silicate gel, and drying in a vacuum drying box to obtain the hydrated calcium silicate early strength agent. After the hydrated calcium silicate early strength agent prepared by the preparation method is mixed with cement, the hydration of cement can be promoted, the setting time of cement is obviously shortened, the early strength of cement is improved, and the hydrated calcium silicate early strength agent has important practical application value in the building field.

Description

technical field [0001] The invention relates to the technical field of building materials, in particular to a calcium silicate hydrate early strength agent and a preparation method thereof. Background technique [0002] With the development of urban infrastructure construction, the construction of prefabricated houses, urban subway tunnels and other engineering projects is booming. Such projects with fast construction progress have higher requirements for the strength of concrete prefabricated components. Therefore, how to improve the early strength of concrete prefabricated components is the key to technology. Calcium Silicate Hydrate CaO·SiO 2 ·nH 2 O(C-S-H), as the most important hydration product in cement-based materials, is also the most important source of improving the strength of concrete. [0003] Patent CN 108249806 A discloses a preparation method of calcium silicate hydrate early strength agent and a self-compacting concrete. The combination of methyl ammoni...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C01B33/24C04B22/08C04B103/12
CPCC01B33/24C04B22/00C04B2103/12
Inventor 朱少宏方云辉柯余良张小芳钟丽娜吴传灯郭元强林添兴
Owner KZJ NEW MATERIALS GROUP CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products