Preparation method and application of multifunctional biomass wrinkle resisting and removing agent

A biomass, multi-functional technology, applied in the field of daily chemicals, can solve problems such as toxicity, and achieve the effect of wrinkle smoothing, wrinkle prevention and anti wrinkle performance improvement

CN110777536AInactive Publication Date: 2020-02-11JIANGNAN UNIV
5 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Current Assignee / Owner
Publication Date
2020-02-11
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 1
    Figure 1
Patent Text Reader

Abstract

The invention discloses a preparation method and application of a multifunctional biomass wrinkle resisting and removing agent and belongs to the technical field of daily chemicals. The agent is composed of, by weight, 2.5-7.5 parts of multifunctional biomass penetrant, 1-3 parts of natural plant essential oil, 1.5-4.5 parts of multifunctional biomass film former and 85-95 parts of solvent. Bio-based raw materials are adopted to prepare the agent, so that the agent is nontoxic and degradable, integrates functions of wrinkle resisting and removing, can be widely applied to wrinkle resisting andremoving of textiles and paper products and even flatting and fixing of hair style and has certain antibacterial function.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to a preparation method and application of a multifunctional biomass anti-wrinkle and wrinkle-removing agent, belonging to the technical field of daily chemicals. Background technique

[0002] Untreated fabrics are prone to wrinkles during use, which affects the appearance. With the improvement of modern living standards and aesthetic needs, people begin to pay more and more attention to the maintenance of personal image. Among them, the cleanliness and width of clothing The texture has a decisive influence on the overall appearance. Therefore, realizing the anti-wrinkle and wrinkle-removing finishing of fabrics has become an important expectation of people and has huge market potential.

[0003] In addition, paper products are also prone to wrinkles due to moisture, improper mechanical force, etc. during transportation, storage and use, affecting the sensory perception and even collection value. Their anti-wrinkle and anti-wrinkl...

Examples

Embodiment 1

[0038] Add 0.5 part of alkyl polyglycoside quaternary ammonium salt, 0.75 part of sucrose fatty acid ester quaternary ammonium salt, 0.75 part of starch ether base quaternary ammonium salt, 0.25 part of rosemary essential oil, 0.75 part of ylang ylang essential oil, lavender After 0.4 parts of essential oil, 0.6 parts of ginger essential oil, 35 parts of deionized water, 5 parts of ethanol, and 2.5 parts of glycerin, use a homogenizer to homogenize at 6500 rpm for 8 minutes. 0.75 parts of ammonium salt, 1.125 parts of sucrose fatty acid ester quaternary ammonium salt, 1.125 parts of starch ether base quaternary ammonium salt, 1.75 parts of guar gum, 1.25 parts of gum arabic, 40 parts of deionized water, 5 parts of ethanol, 2.5 parts of glycerin, and use The homogenizer was homogenized at 3600 rpm for 15 minutes to obtain a translucent microemulsion, which is a multifunctional biomass anti-wrinkle and anti-wrinkle agent.

[0039]Test results: the wrinkle recovery angles of cott...

Embodiment 2

[0041] Add 0.6 parts of alkyl polyglycoside quaternary ammonium salt, 0.65 part of sucrose fatty acid ester quaternary ammonium salt, 0.5 part of starch ether base quaternary ammonium salt, 0.5 part of rosemary essential oil, 0.75 part of ylang-ylang essential oil, lavender After 0.25 parts of essential oil, 0.75 parts of ginger essential oil, 35 parts of deionized water, 5 parts of ethanol, and 2.5 parts of glycerin, use a homogenizer to homogenize at 6500 rpm for 8 minutes. After obtaining a clear solution, continue to add alkyl polyglycosides in sequence. 0.75 parts of ammonium salt, 1.125 parts of sucrose fatty acid ester quaternary ammonium salt, 1.125 parts of starch ether base quaternary ammonium salt, 2 parts of guar gum, 1 part of gum arabic, 40 parts of deionized water, 5 parts of ethanol, 2.5 parts of glycerin, and use The homogenizer was homogenized at 3600 rpm for 15 minutes to obtain a translucent microemulsion, which is a multifunctional biomass anti-wrinkle and ...