Manufacturing method of wall sound insulation material
A technology of sound insulation material and manufacturing method, which is applied to the manufacturing field of wall sound insulation materials, can solve the problems of insufficient adhesion, cracks, peeling, etc. sexual effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] An embodiment provided by the present invention: a method for manufacturing a wall sound insulation material, comprising the following steps:
[0031] S1: separate the bark and the stem of the branch obtained, soak the bark and the stem in clear water respectively, the soaking time of the bark is shorter than the soaking time of the stem, the soaking time of the bark is 8-15 hours, The soaking time of the stem is 12-20 hours, and the soaking temperature is 50°C, then the soaked bark is scraped off the surface juice and impurities, the soaked stem is beaten, and the treated bark and The surface of the stem is dehydrated and dried, the temperature of the drying treatment is 60°C, and then put into the crushing equipment for crushing, using a two-stage crushing scheme, first crushed to 20-50 mesh, soaked in clean water and then soaked for 1-2 hours, then dehydrate and dry the surface, and finally carry out secondary crushing, crushing the bark and stems to 120-170 mesh, av...
Embodiment 2
[0041] An embodiment provided by the present invention: a method for manufacturing a wall sound insulation material, comprising the following steps:
[0042] S1: separate the bark and the stem of the branch obtained, soak the bark and the stem in clear water respectively, the soaking time of the bark is shorter than the soaking time of the stem, the soaking time of the bark is 8-15 hours, The soaking time of the stem is 12-20 hours, and the soaking temperature is 50°C, then the soaked bark is scraped off the surface juice and impurities, the soaked stem is beaten, and the treated bark and The surface of the stem is dehydrated and dried, the temperature of the drying treatment is 60°C, and then put into the crushing equipment for crushing, using a two-stage crushing scheme, first crushed to 20-50 mesh, soaked in clean water and then soaked for 1-2 hours, then dehydrate and dry the surface, and finally carry out secondary crushing, crushing the bark and stems to 120-170 mesh, av...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com