Modified asphalt binder material using crumb rubber and methods of manufacturing a modified asphalt binder
An asphalt adhesive and modified asphalt technology, which is applied in asphalt coatings, building insulation materials, building structures, etc., can solve problems related to adhesive storage, increase in rotational viscosity, etc., and achieve improved resistance to permanent deformation and improved performance , Improve the effect of consistency and performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] Heating pure bitumen to a temperature of about 120°C to about 200°C
[0030] - Addition of about 0.5 wt% to about 5 wt% of one or more synthetic polymers
[0031] Use a high shear mixer for about 5 minutes to about 10 hours
[0032] Add about 0.5wt% to about 10wt% of granular raw rubber
[0033] Use a high shear mixer for about 5 minutes to about 10 hours
[0034] Addition of one or more acids from about 0.5 wt% to about 3 wt%
[0035] Mix the resulting modified bitumen using a low shear mixer for 5 minutes to 48 hours
Embodiment 2
[0037] ·Heating pure bitumen to a temperature of about 120°C to about 200°C
[0038] - Addition of about 0.5 wt% to about 5 wt% of one or more synthetic polymers
[0039] Use a high shear mixer for about 5 minutes to about 10 hours
[0040] Addition of one or more acids from about 0.5 wt% to about 3 wt%
[0041] Use a high shear mixer for about 5 minutes to about 10 hours
[0042] Add about 0.5wt% to about 10wt% of granular raw rubber
[0043] Use a high shear mixer for about 5 minutes to about 10 hours
[0044] Mix the resulting modified bitumen using a low shear mixer for 5 minutes to 48 hours
Embodiment 3
[0046] Heating pure bitumen to a temperature of about 120°C to about 200°C
[0047] Add about 0.5wt% to about 10wt% of granular raw rubber
[0048] Use a high shear mixer for about 5 minutes to about 10 hours
[0049] - Addition of about 0.5 wt% to about 5 wt% of one or more synthetic polymers
[0050] Use a high shear mixer for about 5 minutes to about 10 hours
[0051] Addition of one or more acids from about 0.5 wt% to about 3 wt%
[0052] Mix the resulting modified bitumen using a low shear mixer for 5 minutes to 48 hours
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com