A coal-fired catalyst and high-efficiency technology, applied in physical/chemical process catalysts, metal/metal oxide/metal hydroxide catalysts, fuels, etc., can solve instability, low desulfurization efficiency of sulfur-fixing coal-fired additives, and environmental pollution and other problems, to achieve the effect of improving heat loss, reducing fly ash and dust, and reducing the degree of environmental damage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Embodiment 1 provides a high-efficiency coal-fired catalyst, which is mainly composed of the following ingredients mixed according to mass percentage: potassium salt: 20-40%, industrial-grade sodium chloride: 10-25%, quicklime: 15-30% , bauxite: 9-15%, rare earth element: 1-4%, ferric oxide: 0.1-1%, mix the above ingredients evenly, and then get this high-efficiency coal-burning catalyst.
[0019] The potassium salt is nitrate or carbonate.
[0020] The bauxite can be obtained by directly pulverizing bauxite.
[0021] The ferric oxide may be a trace amount of ferric oxide contained in bauxite.
[0022] The rare earth elements may be rare earth oxides or rare earth chlorides.
Embodiment 2
[0023] Embodiment 2 provides a method for using the high-efficiency coal-fired catalyst. Take 35 parts of potassium nitrate, 25 parts of industrial grade sodium chloride, 24 parts of quicklime, 15 parts of bauxite, and 1 part of rare earth according to the mass percentage, and grind Mix evenly to obtain the high-efficiency coal-burning catalyst, and then mix the high-efficiency coal-burning catalyst, high-quality coal, and water in a ratio of 1:1000:100 by mass percentage.
Embodiment 3
[0024] Embodiment 3 provides a method for using the high-efficiency coal-fired catalyst. Take 33 parts of potassium nitrate, 25 parts of industrial grade sodium chloride, 25 parts of quicklime, 15 parts of bauxite, and 2 parts of rare earth according to the mass percentage, and grind Mix evenly to obtain the high-efficiency coal-burning catalyst, and then mix the high-efficiency coal-burning catalyst, high-quality coal, and water in a ratio of 1:1000:100 by mass percentage.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com