Surface printed solidified matte ink and preparation method thereof
A matte ink and ink technology, applied in inks, household appliances, applications, etc., can solve the problems of the matte film being difficult to achieve precise hollowing, unable to achieve the embellishment effect, etc., to achieve obvious matte effect, highlight the decoration grade, and reduce production. cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] A surface printing solidified matte ink, which is formed by mixing an ink base material with a curing agent in a proportion of 6-10%, and the components of the ink base material are formulated in weight percent as follows:
[0012] 23 n-propyl esters, 10 butyl acetates, 8 polyurethane resins, 10 aldehyde and ketone resins, 1 leveling agent, 40 nitrocellulose pulp, 7 ternary chlorinated vinegars, 0.5 defoamers, and 0.5 dispersants.
[0013] The composition of above raw material is 100 parts.
[0014] The preparation method is to grind and dissolve the above-mentioned n-propyl ester, butyl acetate, polyurethane resin, ternary chlorinated vinegar, and aldehyde and ketone resin for 4-6 hours, and the fineness is less than 15um; Slurry and disperse at a high speed at a speed of 900-1500r / min, and disperse at a high speed for 4 hours; filter after re-inspection, and the net pattern is less than 120 mesh; after the acceptance, the finished product is packaged to obtain the ink...
Embodiment 2
[0016] A surface printing solidified matte ink, which is formed by mixing an ink base material with a curing agent in a proportion of 6-10%, and the components of the ink base material are formulated in weight percent as follows:
[0017] 20 n-propyl esters, 11 butyl acetates, 7 polyurethane resins, 8 aldehyde and ketone resins, 0.5 leveling agents, 45 nitrate pulp, 8 ternary chlorinated vinegars, 0.2 defoamers, and 0.3 dispersants.
[0018] The composition of above raw material is 100 parts.
[0019] The preparation method is the same as in Example 1, so details are not repeated.
Embodiment 3
[0021] A surface printing solidified matte ink, which is formed by mixing an ink base material with a curing agent in a proportion of 6-10%, and the components of the ink base material are formulated in weight percent as follows:
[0022] 26 n-propyl esters, 13 butyl acetates, 5 polyurethane resins, 12 aldehyde and ketone resins, 1.5 leveling agents, 35 nitrate pulp, 7 ternary chlorinated vinegars, 0.3 defoamers, and 0.2 dispersants
[0023] The composition of above raw material is 100 parts.
[0024] The preparation method is the same as in Example 1, so details are not repeated.
[0025] The performance physical and chemical index test table of above-mentioned each embodiment gained surface printing curing matte ink is as follows:
[0026] --
[0027] It can be seen from the test results in the table that the surface printing cured matte ink obtained in the embodiment of the present invention has excellent touch, pressure resistance, light fastness, yellowing resistance,...