A method of knitting gloves
A glove and covering technology, which is applied in the field of woven gloves, can solve the problems of wear resistance, cut resistance, tear resistance and puncture resistance of safety protective gloves, and achieve low cost effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0045] A kind of method for knitting gloves that present embodiment relates to, comprises the steps:
[0046] One, prepare the first covered yarn and the second covered yarn respectively;
[0047] The preparation method of the first covering yarn is:
[0048] S1. With 100D glass fiber and 0.05mm steel wire as the first core wire, the first core wire is covered with 200D polyethylene fiber after winding to obtain the first covered yarn semi-finished product. For 100 twists, the twist direction is Z twist, and the crimp coefficient of the first covered yarn semi-finished product is 99.8;
[0049] S2. The first covered yarn semi-finished product obtained in step S1 is used as the second core thread, and the second core thread is covered with 100D polyester yarn and 32 cotton yarns after winding to obtain the first covering Yarn, the twist of the 100D polyester filament when covering is 530 twists, the twist direction is Z twist, the twist of the 32 cotton yarns is 240 twists, a...
Embodiment 2
[0060] A kind of method for knitting gloves that present embodiment relates to, comprises the steps:
[0061] One, prepare the first covered yarn and the second covered yarn respectively;
[0062] The preparation method of the first covering yarn is:
[0063] S1. With 100D glass fiber and 0.05mm steel wire as the first core wire, the first core wire is covered with 200D polyethylene fiber after winding to obtain the first covered yarn semi-finished product. For 100 twists, the twist direction is Z twist, and the crimp coefficient of the first covered yarn semi-finished product is 99.8;
[0064] S2. The first covered yarn semi-finished product obtained in step S1 is used as the second core thread, and the second core thread is covered with 100D polyester yarn and 32 cotton yarns after winding to obtain the first covering Yarn, the twist of the 100D polyester filament when covering is 530 twists, the twist direction is Z twist, the twist of the 32 cotton yarns is 240 twists, a...
Embodiment 3
[0075] A kind of method for knitting gloves that present embodiment relates to, comprises the steps:
[0076] One, prepare the first covered yarn and the second covered yarn respectively;
[0077] The preparation method of the first covering yarn is:
[0078] S1. With 100D glass fiber and 0.05mm steel wire as the first core wire, the first core wire is covered with 200D polyethylene fiber after winding to obtain the first covered yarn semi-finished product. For 100 twists, the twist direction is Z twist, and the crimp coefficient of the first covered yarn semi-finished product is 99.8;
[0079] S2. The first covered yarn semi-finished product obtained in step S1 is used as the second core thread, and the second core thread is covered with 100D polyester yarn and 32 cotton yarns after winding to obtain the first covering Yarn, the twist of the 100D polyester filament when covering is 530 twists, the twist direction is Z twist, the twist of the 32 cotton yarns is 240 twists, a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com