[0018] The method for making old furniture includes the following steps:
[0019] a. Impregnation: add kaolin and water to form a mud with a weight ratio of 30%, immerse the furniture made of jujube wood in the mud for 30 minutes, take out and remove the mud attached to the furniture; mix 1 with 5 parts of 20% hydrogen peroxide Use 18% ammonia water to form a mixed solution, use the mixed solution to brush the outer surfaces of the furniture 20 times, and the brushing environment temperature is 30 degrees Celsius; use 30% alcohol solution to brush the furniture surface 3 times ;Use charcoal fire to bake at 60 degrees Celsius for 5 minutes;
[0020] b. Filling the vacancy: use plasticine to fill the defect of the furniture to make the surface of the furniture smooth;
[0021] c. Surface treatment: Use 50# sandpaper to finely grind the surface of the furniture, and then use 100# sandpaper to roughen the surface of the furniture;
[0022] d. Digging grooves to form initial, med...
Embodiment 2
[0029] The method for making old furniture includes the following steps:
[0030] a. Impregnation: add kaolin and water to prepare mud with a weight ratio of 40%, immerse the furniture made of Chinese toon wood in the mud for 50 minutes, take out and remove the mud attached to the furniture; mix with 9% hydrogen peroxide with a concentration of 28% 1 part of ammonia water with a concentration of 20% forms a mixed solution. Use the mixed solution to brush the outer surfaces of the furniture 30 times. The ambient temperature for painting is 60 degrees Celsius; use an alcohol solution with a concentration of 50% to brush the surface of the furniture for 5 times; using charcoal fire at 80 degrees Celsius for 8 minutes;
[0031] b. Filling the vacancy: use plasticine to fill the defect of the furniture to make the surface of the furniture smooth;
[0032] c. Surface treatment: Use 70# sandpaper to finely grind the surface of the furniture, and then use 150# sandpaper to roughen th...
Embodiment 3
[0040] The method for making old furniture includes the following steps:
[0041] a. Impregnation: add kaolin and water to form a mud with a weight ratio of 35%, immerse the furniture made of mahogany in the mud for 40 minutes, take out and remove the mud attached to the furniture; mix 1 part with 6 parts of 22% hydrogen peroxide A mixed solution of ammonia water with a concentration of 19% is formed, and the mixed solution is used to brush the outer surfaces of the furniture 26 times at a temperature of 50 degrees Celsius; the alcohol solution with a concentration of 40% is used to brush the surface of the furniture 4 times; Bake at 70°C for 6 minutes using charcoal fire;
[0042] b. Filling the vacancy: use plasticine to fill the defect of the furniture to make the surface of the furniture smooth;
[0043] c. Surface treatment: use 60# sandpaper to finely grind the surface of the furniture, and then use 120# sandpaper to roughen the surface of the furniture to make the surf...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com