A technology for plastic film, packaging and printing, applied in detergent compositions, detergent compounding agents, detergent composition solvents, etc., can solve the problems of a large number of foams, not easy to dissipate, and the degumming agent consumes a large film, and achieves low volatility. , Shorten the degumming time, not easy to delaminate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Example Embodiment
[0030] Example 1:
[0031] At room temperature, add 20.0g of benzyl alcohol, 20.0g of ethylene glycol, 0.2g of sodium cetylbenzene sulfonate, 1.0g of emulsified silicone oil and 58.8g of water into a clean 250ml beaker, and stir for 2 minutes Until fully mixed and uniform, 100 g of the degumming agent of the present invention is obtained.
[0032] Put the aluminum-plated film sample with the aluminum-plated layer and composite adhesive on the surface into the prepared degumming agent, and scrape off by friction. The adhesive layer can be easily scraped off in 10 seconds at room temperature to expose the bright surface of the aluminum-plated layer. The degumming agent was recycled for 30 minutes in the washing machine, and only a small amount of foam was produced.
Example Embodiment
[0033] Example 2
[0034] At room temperature, add 33.0g of benzyl alcohol, 33.0g of N-methylpyrrolidone, 0.5g of cetyltrimethylammonium bromide, 1.5g of polyoxypropylene glyceryl ether and 32.0 to a clean 250ml beaker. g of water, stirred for 2 minutes until fully mixed uniformly, to obtain 100 g of the degumming agent of the present invention.
[0035] Put the aluminum-plated film sample with the aluminum-plated layer and composite adhesive on the surface into the prepared degumming agent, and scrape it off by friction. The adhesive layer can be easily scraped off in 6 seconds at room temperature to expose the bright surface of the aluminum-plated layer. The degumming agent was recycled for 30 minutes in the washing machine, and only a small amount of foam was produced.
Example Embodiment
[0036] Example 3
[0037] At room temperature, add 39.0g of phenethyl alcohol, 38.2g of n-propanol, 0.8g of cetyltrimethylammonium bromide, 2.0g of polyoxypropylene polyoxyethylene glyceryl ether and 20.0g of water is stirred for 2 minutes until fully mixed uniformly to obtain 100g of the degumming agent of the present invention.
[0038] Put the aluminized film sample with aluminized layer and composite glue on the surface of the prepared degumming agent, and scrape it off by friction. The glue layer can be easily scraped off in 12 seconds at room temperature to expose the bright surface of the aluminized layer. The degumming agent was recycled for 30 minutes in the washing machine, and only a small amount of foam was produced.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap