A kind of nano energy storage fuel and preparation method thereof
A nanometer and energy storage technology, applied in fuel, liquid carbon-containing fuel, petroleum industry, etc., can solve problems affecting fuel performance, complex coating process, and affecting fuel energy performance, etc., to achieve excellent anti-settling performance and good combustion performance , stable long-term storage effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Under the protection of high-purity argon in the glove box, fully mix 0.3g of high-activity nano-Al powder with 0.7g of ortho-substituted hexylcarborane. After sealing, use an ultrasonic cleaning agent for 30 minutes to form a uniform slurry, and place it for more than 24 hours , add 9g JP-10, mix well to make nano energy storage fuel. Pour the fuel into a 5# centrifuge tube (10ml), centrifuge at a high speed of 6500r / min for 10 minutes, the fuel is uniform without sedimentation. Measured fuel density: 0.96g / cm 3 , Volume calorific value: 41.3MJ / L.
Embodiment 2
[0028] Under the protection of high-purity argon in the glove box, fully mix 3.0g of high-activity nano-Al powder and 6.0g of ortho-substituted hexylcarborane, after sealing, use ultrasonic cleaning agent for 30min to form a uniform slurry, and place it for more than 24h , add 1g JP-10, mix well to make nano energy storage fuel. Pour the fuel into a 5# centrifuge tube (10ml), centrifuge at a high speed of 6500r / min for 10 minutes, the fuel is uniform without sedimentation. Measured fuel density: 1.13g / cm 3 , Volume calorific value: 50.6MJ / L.
Embodiment 3
[0030] Under the protection of high-purity argon in the glove box, fully mix 0.5g of high-activity nano-Al powder with 9g of ortho-substituted hexylcarborane, seal it, and use an ultrasonic cleaning agent for 15 minutes to form a uniform slurry, and place it for more than 2 hours. Add 0.5g JP-10, mix well to make nano energy storage fuel. Pour the fuel into a 5# centrifuge tube (10ml), centrifuge at a high speed of 6500r / min for 10 minutes, the fuel is uniform without sedimentation. Measured fuel density: 0.93g / cm 3 , Volume calorific value: 46.2MJ / L.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
density | aaaaa | aaaaa |
heating value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com