A supramolecular hydrogel and chiral technology, applied in skin diseases, ointment delivery, medical preparations containing active ingredients, etc., can solve problems such as long course of disease, many complications, affecting the health and quality of life of patients, and achieve The ingredients are smooth and moisturizing, it can be used in a wide range of places, and it can maintain the antibacterial and repairing effect for a long time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0013] Ointment formulation:
[0014]
[0015] Preparation process: take the chiral supramolecular hydrogel factor in a container and dissolve it in pure water at 80-90°C for 5 minutes; take another grain worm extract and add pure water and stir it at room temperature for 10 minutes to dissolve; take borneol and add pure water at 60-80°C and stir until completely dissolved; take another natural beeswax and liquid paraffin in another container, and heat at 40-50°C until completely melted. Finally, slowly add the water phase liquid into the oil phase liquid and mix, and keep stirring until the final shape is obtained.
Embodiment 2
[0017] Ointment formulation:
[0018]
[0019] Preparation process: take the chiral supramolecular hydrogel factor in a container and dissolve it in pure water at 80-90°C for 5 minutes; take another grain worm extract and add pure water and stir it at room temperature for 10 minutes to dissolve; take borneol and add pure water at 60-80°C and stir until completely dissolved; take another natural beeswax and liquid paraffin in another container, and heat at 40-50°C until completely melted. Finally, slowly add the water phase liquid into the oil phase liquid and mix, and keep stirring until the final shape is obtained.
Embodiment 3
[0021] Ointment formulation:
[0022]
[0023] Preparation process: take the chiral supramolecular hydrogel factor in a container and dissolve it in pure water at 80-90°C for 5 minutes; take another grain worm extract and add pure water and stir it at room temperature for 10 minutes to dissolve; take borneol and add pure water at 60-80°C and stir until completely dissolved; take another natural beeswax and liquid paraffin in another container, and heat at 40-50°C until completely melted. Finally, slowly add the water phase liquid into the oil phase liquid and mix, and keep stirring until the final shape is obtained.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com