Mold type sludge curing agent
A technology of curing agent and sludge, which is applied in the field of mold-type sludge curing agent, can solve the problem of secondary damage to the environment and achieve the effect of avoiding secondary damage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0007] A mold-type sludge curing agent, the raw materials in the formula are composed by weight percentage: 0.5% fly ash, 10% potassium hydroxide, 1% silicon dioxide, 1% carbide slag, 1% surfactant, 5% Calcium lignosulfonate, 10% sodium lignosulfonate, 30% sodium carbonate, at this time the effect of solidifying the sludge is not ideal.
Embodiment 2
[0009] A mold-type sludge curing agent, the raw materials in the formula are composed by weight percentage: 6% fly ash, 35% potassium hydroxide, 10% silicon dioxide, 3% carbide slag, 2.5% surfactant, 20% Calcium lignosulfonate, 20% sodium lignosulfonate, and 60% sodium carbonate will cause secondary damage to the environment to a certain extent.
Embodiment 3
[0011] A mold-type sludge solidifying agent, the raw materials in the formula are composed by weight percentage: 4% fly ash, 23% potassium hydroxide, 5% silicon dioxide, 1.5% carbide slag, 1.25% surfactant, 13% Calcium lignosulfonate, 15% sodium lignosulfonate, 45% sodium carbonate, at this time can avoid secondary damage to the environment while having excellent solidification sludge.
PUM
Login to View More Abstract
Description
Claims
Application Information