Construction method of a pool
A construction method and pool technology, applied in swimming pools, gymnasiums, building types, etc., can solve the problems of high maintenance cost of pools, fluctuations in anti-freezing performance, easy cracking of pools, etc. Enhanced ability, less cracking effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0072] A kind of construction method of pond, with reference to figure 1 , including the following specific steps:
[0073] S1. Foundation pit excavation, details are as follows:
[0074] Determine and mark the construction position of the pool according to the design drawings, and excavate the foundation pit for the construction of the water supply pool according to the marked position.
[0075] S2. Template installation, as follows:
[0076] Clean the inner wall and bottom of the foundation pit and tamp it. Drill some drain holes along the edge of the foundation pit with an electric drill. The depth of the drain hole is 3m, and the diameter of the drain hole is 3cm. Insert a drain pipe into the drain hole. The outer diameter is consistent with the inner diameter of the drainage hole, and then the foundation cushion is laid on the bottom of the foundation pit. The foundation cushion is soft soil. After the foundation cushion is laid, the steel skeleton is built according to...
Embodiment 2
[0088] The difference with embodiment 1 is:
[0089] The depth of the drainage hole in S2 is 4m;
[0090] Wherein, the preparation method of concrete slurry is as follows:
[0091] a. Add 100kg of slag cement and 90kg of water into the stirred tank, the rotating speed of the stirred tank is 75r / min, stir for 10min, the temperature is 50-60°C, and stir evenly to form a primary mixture;
[0092] b. Add N-methyl-3,3-diphenylpropylamine 5kg, 4-(1-phenylethyl)resorcinol 3kg and silane coupling agent 0.7kg in the stirred tank, the rotating speed of the stirred tank is 60r / min, stirring for 8min, the temperature is 50-55℃, stirring evenly to form an intermediate mixture;
[0093] c. Add 350kg of coarse aggregate and 250kg of fine aggregate into the stirring tank, the rotating speed of the stirring tank is 70r / min, stir for 15min, the temperature is 60-65°C, and stir evenly to form concrete slurry.
Embodiment 3
[0095] The difference with embodiment 1 is:
[0096] The depth of the drainage hole in S2 is 5m;
[0097] Wherein, the preparation method of concrete slurry is as follows:
[0098] a. Add 100kg of slag cement and 100kg of water into the stirred tank, the rotating speed of the stirred tank is 75r / min, stir for 10min, the temperature is 50-60°C, and stir evenly to form a primary mixture;
[0099] b. Add 6 kg of N-methyl-3,3-diphenylpropylamine, 4 kg of 4-(1-phenylethyl) resorcinol and 1 kg of silane coupling agent in the stirred tank, and the rotating speed of the stirred tank is 60r / min, stir for 8min, the temperature is 50-55°C, stir evenly to form an intermediate mixture;
[0100] c. Add 400kg of coarse aggregate and 300kg of fine aggregate into the stirring tank, the rotating speed of the stirring tank is 70r / min, stir for 15min, the temperature is 60-65°C, and stir evenly to form concrete slurry.
PUM
| Property | Measurement | Unit |
|---|---|---|