An antibacterial and antifungal agent and polyion technology, which is applied in the field of polyionic antibacterial antifungal agent and its preparation, can solve the problems of environmental pollution deterioration and chemical harm, and achieve low cost, fast action, and enhanced sterilization and antifungal properties. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] A multi-ion antibacterial and antifungal agent, wherein the calcium ion content is 950mg / L, the potassium ion content is 120mg / L, the magnesium ion content is 52mg / L, the iron ion content is 1.2mg / L, and deionized water.
[0025] The preparation method is as follows: 1) Weigh calcium chloride, potassium chloride and magnesium sulfate respectively according to the concentration of each ion, add magnesium sulfate into deionized water, stir for 1 hour, and then add calcium chloride and magnesium sulfate successively. Potassium chloride, stirred and reacted at 60°C for 4 hours;
[0026] 2) Weighing ferric sulfate according to the concentration of iron ions, adding it to the ionic liquid obtained in step 1), stirring and reacting at 60° C. for 1 hour;
[0027] 3) Stir the ionic liquid obtained in step 2) to react at room temperature for 10 hours, let it stand for 48 hours, and take the supernatant to obtain the multi-ionic antibacterial and antifungal agent.
Embodiment 2
[0029] A multi-ion antibacterial and antifungal agent, wherein the content of calcium ions is 1150mg / L, the content of potassium ions is 100mg / L, the content of magnesium ions is 90mg / L, the content of iron ions is 0.5mg / L, the content of boron ions is 0.6mg / L, and deionized water.
[0030] The preparation method is: 1) Weigh the plaster of paris, potassium sulfate and sodium tetraborate respectively according to the concentration of each ion, add the sodium tetraborate into the weighed deionized water, stir for 1 hour, and then add the plaster of paris and sulfuric acid in turn Potassium, stirred and reacted at 45°C for 6 hours;
[0031] 2) Weighing ferric sulfate according to the concentration of iron ions, adding it to the ionic liquid obtained in step 1), stirring and reacting at 45° C. for 2 hours;
[0032] 3) Weigh magnesium carbonate according to the concentration of magnesium ions, add it to the ionic liquid obtained in step 2), react at room temperature for 10 hours ...
Embodiment 3
[0034] A multi-ion antibacterial and antifungal agent, wherein the content of calcium ions is 800mg / L, the content of potassium ions is 180mg / L, the content of magnesium ions is 150mg / L, the content of iron ions is 1.9mg / L, the content of boron ions is 0.35mg / L, and deionized water.
[0035] The preparation method is: 1) Weigh calcium chloride, potassium chloride and boric acid respectively according to the concentration of each ion, add boric acid into the weighed deionized water, stir for 1.5 hours, and then add calcium chloride and chloride Potassium, stirred and reacted at 50°C for 4 hours;
[0036] 2) Weighing ferric sulfate according to the concentration of iron ions, adding it to the ionic liquid obtained in step 1), stirring and reacting at 50° C. for 2 hours;
[0037] 3) Weigh magnesium carbonate according to the concentration of magnesium ions, add it to the ionic liquid obtained in step 2), react at room temperature for 10 hours under stirring, let it stand for 48 ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology