Waterborne polyurethane dispersion, preparation method thereof and sunscreen cosmetic composition
A cosmetic composition, water-based polyurethane technology, applied in the field of personal care, can solve problems such as unpleasant odor, unsatisfactory, weak ability to increase SPF value, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0110] The formula is shown in Table 1 below, and its preparation method includes the following steps: according to the proportion, homogenize components d and e at 78°C at a speed of 6000r / min for 10 minutes, and homogenize phases a, c and h at room temperature at 500r / min , Add phases d, e and component b to phases a, c, h, homogenize at 6000r / min for 10 minutes, then add components f and g under slow stirring at 500r / min, and stir for 15 minutes.
[0111] See Table 2 for the evaluation results.
[0112] Table 1 embodiment and comparative example raw material mass parts
[0113] Example 1 Example 2 Example 3 Example 4 Example 5 Comparative example 1 Comparative example 2 Comparative example 3 Comparative example 4 Comparative example 5 Waterborne Polyurethane Dispersion-1 5 0 0 0 0 0 0 0 0 0 Waterborne Polyurethane Dispersion-2 0 3 0 0 0 0 0 0 0 0 Waterborne Polyurethane Dispersion-3 0 0 8 0 0 0 0 0 0 ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com