Stretchable adhesive film and display device comprising same
A display device, adhesive film technology, applied in the direction of transportation and packaging, film/sheet adhesive, adhesive type, etc., can solve difficult recovery, adhesive and substrate do not have stretchability and strain Characteristics and other issues, to achieve the effect of excellent ability, excellent durability, and excellent adhesive strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment approach
[0126] Hereinafter, the present disclosure will be described in detail with reference to the embodiments so that those skilled in the art can easily implement the present disclosure. However, the present disclosure can be presented in various forms and is not limited to the embodiments described herein.
preparation example
[0128] The components, weight ratios, and thicknesses of the base layer and the first adhesive layer of the stretchable adhesive films used as Examples and Comparative Examples of the present application are described in Table 1 below.
[0129] [Table 1]
[0130]
[0131] In Table 1, Dow Corning's Xiameter 9050 30P material was used as the liquid silicone rubber (LSR), which means that, as a two-component type, the main components were mixed in ratios of 20:1, 10:1 and 5:1 respectively. Divided into A (Part A) and Curing Agent B (Part B), TPU means a polyurethane-based material that is a product of LG Chem.
Embodiment 1
[0133] As a base layer, the components described in Example 1 of Table 1 were mixed in the described weight ratio, and the resultant was stirred and defoamed. After that, the mixed solution was coated on the fluorine release surface of TACS's TS502 (fluorine-based release film), and then the resultant was dried in an oven at 150°C for 5 minutes so that the final thickness became Example 1 of Table 1 The thickness described in.
[0134]After that, as the first adhesive layer, a curing agent was added to the acrylic resin in which the components described in Example 1 of Table 1 were polymerized at the described weight ratio, and then methyl ethyl ketone (MEK) was added thereto so that The solid content became 20%, and the resultant was stirred and defoamed. After that, the mixed solution was coated on the silicone release surface of RF02N (silicone release film) of SKC hi-tech & marketing (formerly SKCHaas), and the resultant was dried in an oven at 120°C for 3 minutes so that...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com