preparation example Construction
[0075] In the present invention, the preparation method of the adhesive layer comprises the following steps: under the protection of an inert gas, mix the tackifying resin and the plasticizer, and heat to fully melt while stirring; then continue heating to 180-240°C, Add styrene-based thermoplastic elastomer, silicone resin and antioxidant, and continue to stir for 2-5 hours; stop stirring, cool down to room temperature, coat, and cure.
[0076] The second aspect of the present invention provides the application of the packaging roll film with a locking structure, which is applied in the field of agricultural products.
Embodiment 1
[0081] Embodiment 1 provides a packaging roll film with a locking structure, the packaging roll film is formed by connecting several packaging segments end-to-end through a locking structure 3; between the packaging segment and the locking structure 3 is Fixedly connected; the locking structure is made of a base material 31, an adhesive layer 32 and a release layer 33; the base material 31 and the release layer 33 are bonded and connected by the adhesive layer 32; in the locking structure 3, the base The lengths of the material 31 and the release layer 33 are not less than the length of the adhesive layer 32; the packaging section includes a non-adhesive area 1 and an adhesive area 2; the non-adhesive area 1 and the adhesive area 2 are fixedly connected; the adjacent Between the packaging sections, the adhesive zone 2 of the previous packaging section and the non-adhesive zone 1 of the subsequent packaging section are connected by a locking structure 3; 1 is a fixed connection...
Embodiment 2
[0090] The difference between embodiment 2 and embodiment 1 lies in the adhesive layer.
[0091] The raw materials for the preparation of the adhesive layer include at least the following components in parts by weight: 100 parts of styrene-based thermoplastic elastomer, 10 parts of silicone resin, 80 parts of tackifying resin, 30 parts of plasticizer, and 0.5 parts of antioxidant share.
[0092] The thermoplastic elastomer is a styrene-isoprene-styrene block copolymer, purchased from Guangzhou Qianyiyuan Synthetic Material Technology Co., Ltd., model 1125;
[0093] The silicone resin is bisphenol A modified polymethyl silicone resin; the bisphenol A epoxy resin is purchased from Angsen Building Materials Hebei Co., Ltd., brand E-35; the polymethyl silicone resin is purchased from Hubei New Sihai Chemical Co., Ltd., model SH-9503; the preparation method of the bisphenol A modified polymethyl silicone resin is: add polymethyl silicon to isopropanol at a temperature of 40°C, and...
PUM
| Property | Measurement | Unit |
|---|---|---|
| melt flow index | aaaaa | aaaaa |
| epoxy value | aaaaa | aaaaa |