Apparatus and method for measuring welding tube corrosion under stress condition
Patent Information
- Authority / Receiving Office
- CN Β· China
- Current Assignee / Owner
- BAOSHAN IRON & STEEL CO LTD
- Publication Date
- 2009-03-04
- Estimated Expiration
- Not applicable Β· inactive patent
Smart Images
Figure 1 Figure 2 Figure 3
Abstract
Description
technical field
[0001] The present invention relates to the field of testing or analyzing materials by means of determining their chemical or physical properties, in particular to the field of an electrochemical measurement system for testing atmospheric erosion, corrosion or anticorrosion measurements. Background technique
[0002] At present, the electrochemical method is used to measure the corrosion resistance of the weld seam of the longitudinal seam welded pipe. The electrochemical method generally adopts an electrolytic cell of a three-electrode system, and the weld seam and the base metal are processed into working electrodes, and the anode overpotential 50mV of the constant potential method is used to corrode for 144 hours, and the groove corrosion sensitivity coefficient of the weld seam is measured, with This is used to indicate the corrosion resistance of the weld.
[0003] On the other hand, many welded pipe products, such as J55 welded pipe, K55 welded pipe, e...