Active energy porcelain, preparation method and second-boiling type slightly alkaline fresh boiled water electric heater

An active energy and heater technology, applied in beverage preparation devices, applications, kitchen utensils, etc., can solve problems such as unhealthy water, loss of weak alkalinity, and lack of trace elements, so as to enhance human immunity and improve microcirculation , good cost-effective effect

CN103044015AInactive Publication Date: 2013-04-17舒定涛
3 Cites 1 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2013-04-17
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 1
    Figure 1
  • Figure 2
    Figure 2
  • Figure 3
    Figure 3
Patent Text Reader

Abstract

The invention discloses active energy porcelain, a preparation method and a second-boiling type slightly alkaline fresh boiled water electric heater. The active energy porcelain consists of the following materials in percentage by weight: 10-50% of tourmaline powder, 10-30% of medical stone powder, 1-10% of intermetallic compound powder, 1-15% of calcium sulfite powder and 20-40% of boron-silicon glass powder. Through adopting the invention, the treated water has the advantages that the water does not contain any substance toxic or harmful to human body and with peculiar smell and is rich in mineral substrates necessary to human body, the content of mineral substances is moderate, the PH value shows slight alkalinity, and the water is energetic micro-cluster water and has the media nutrition physiological function of water, namely the dissolving capacity, seepage force, diffusion force, metabolism force, emulsifying force and the like are superior to those of various types of drinking water on the market. The second-boiling type slightly alkaline fresh boiled water electric heater disclosed by the invention also has the advantages of simple structure, strong practicability and operability and great market prospect.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to an active energy porcelain, a production method and a second-boiling type weak alkaline fresh water electric heater. Background technique

[0002] Water is the source of life. The earliest life in the world was born in water. The proportion of water in the tissues of adults is about 70%, the proportion of water in the tissues of middle-aged people is about 60%, and the proportion of water in the tissues of old people The proportion of water accounts for about 50%, of which the water in the blood accounts for about 90%, the water in the brain tissue accounts for about 85%, the water in the muscles accounts for 75%, and the water in the bones accounts for 50%. Moisture can be as high as 80%-90%. If the proportion of water in the human body is lower than 50%, people's lives will be in danger. It can be seen that water is very important to human life.

[0003] If people want to live healthy, they need to drink healthy water. The...

Examples

Embodiment 1

[0066] Embodiment 1 (borosilicate glass, percentage by weight, the same below)

[0067] Silicon dioxide 70%; Diboron trioxide 1%;

[0068] Potassium oxide 0.5%; Calcium oxide 0.3%.

Embodiment 2

[0069] Example 2 (borosilicate glass)

[0070] Silicon dioxide 85%; Diboron trioxide 15%;

[0071] Potassium oxide 2%; Calcium oxide 1%.

Embodiment 3

[0072] Example three (borosilicate glass)

[0073] Silica 95%; Diboron Trioxide 25%;

[0074] Potassium oxide 3%; Calcium oxide 2%.

[0075] Above-mentioned embodiment one to embodiment three, after formulating in proportion, press figure 1 Borosilicate glass powder can be obtained by processing the shown borosilicate glass powder. Specifically, the preparation of borosilicate glass powder comprises the following steps:

[0076] (11) For the preparation of borosilicate glass raw materials, weigh each component according to the ratio of any one of the formulas in Embodiment 1 to Embodiment 3;

[0077] (12) Ball mill mixing, use a ball mill to mix the various components evenly;

[0078] (13) High-temperature melting, melting the mixed raw materials at 1500-1700 degrees Celsius;

[0079] (14) Water quenching into granules, putting the melted borosilicate glass into water in a linear shape, so that the borosilicate glass liquid is cooled in water to form glass granules;

[0...