Compound annular electrode electrostatic spinning device
A ring electrode and electrospinning technology, which is applied in textiles and papermaking, filament/thread forming, fiber processing, etc., can solve the problem of inability to realize 100% utilization of spinning solution, inability to achieve long-term uniform electrospinning, and inability to achieve Solution effective protection and other issues, to reduce high voltage damage to the instrument or harm to the human body, avoid direct contact, the effect of reliable principle
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0011] The main structure of this embodiment includes a motor 1, a liquid brush 2, an insulating tape 3, a metal shaft 4, a metal ring electrode 5, micro-nano fibers 6, a metal collector 7, a high-voltage power supply negative pole 8, an insulating pulley 9, and a high-voltage power supply positive pole 10 , insulating shaft 11, high voltage power supply 12, liquid supply system 13, shunt pipe 14, collecting substrate 15, feeding drum 16 and discharging drum 17; round hanging metal shaft 4 is fixedly installed with 4-8 groups of concentric metal The ring electrode 5 and one end of the metal shaft 4 are electrically connected to the high voltage power supply 12 through the positive pole 10 of the high voltage power supply; 4-8 sets of concentric insulating pulleys 9 are fixedly installed on the insulating shaft 11, and the output shaft of the motor 1 is linked with the insulating shaft 11 and drives All the insulated pulleys 9 rotate, and the insulated pulleys 9 rotate through t...
Embodiment 2
[0013] This embodiment takes polyvinylpyrrolidone PVP solution as an example to describe in detail, set the ambient temperature to 24.5°C, the relative humidity of the environment to 43%RH, and select the polyvinylpyrrolidone PVP solution with a mass percentage of 13% as the spinning solution; One gram of polyvinylpyrrolidone (PVP, its molecular weight is 1.3 million) particles is slowly added to 87 grams of absolute ethanol under magnetic stirring, magnetically stirred at room temperature for 4-5 hours and then left to stand for 0.5-1 hour to obtain uniform and transparent The mass percentage is the PVP electrospinning precursor solution of 13%; Then put the prepared PVP solution into the liquid supply system 13, open the motor 1 that controls the rotation of the insulating pulley 9, and the insulating pulley 9 starts to rotate and passes through the insulating belt 3 drives the metal ring electrode 5 to rotate; then turn on the high-voltage power supply 12 and adjust the volt...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com