A technology of branding and cotton fire, which is applied in decorative arts and crafts for producing decorative surface effects, etc. It can solve the problems of failing to meet environmental protection requirements and harmfulness to the human body, and achieve the effect of simple and practical methods, clear writing or pictures and texts
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Dai cotton fire branding method, set the raised part of the figure or text on the soldering iron, heat the soldering iron to 110 degrees, flatten the Dai cotton, and use the raised part of the soldering iron to burn the Dai cotton for 20 seconds to make a branded Graphic or text Dai cotton wrapping paper. The thickness of Dai cotton is 1mm.
[0023] The preparation method of above-mentioned Dai nationality cotton is:
[0024] (1) Material collection: in July and August every year, peel off the bark of the main trunk or branches of the mulberry tree with a knife, and then remove the green surface layer of the bark;
[0025] (2) drying material: hang the stripped bark inside and outside the yard, dry it and store it for later use;
[0026] (3) Soaking: soak the dry bark in water for 1 day;
[0027] (4) Ash mixing: first sieve the fire ash with a sieve to remove charcoal and other sundries, then place the soaked bark in it, let the fire ash evenly adhere to the bark, an...
Embodiment 2
[0036] A Dai cotton fire branding method. Set the raised parts of graphics or characters on the soldering iron, heat the soldering iron to 180 degrees, flatten the Dai cotton, and use the raised parts of the soldering iron to burn the Dai cotton for 10 seconds. Branded with graphics or text Dai cotton wrapping paper. The thickness of Dai cotton is 0.15mm.
[0037] The preparation method of above-mentioned Dai nationality cotton is:
[0038] (1) Material collection: in July and August every year, peel off the bark of the main trunk or branches of the mulberry tree with a knife, and then remove the green surface layer of the bark;
[0039] (2) drying material: hang the stripped bark inside and outside the yard, dry it and store it for later use;
[0040] (3) soaking: the dried bark is placed in water and soaked for 5 days;
[0041] (4) Ash mixing: first sieve the fire ash with a sieve to remove charcoal and other sundries, then place the soaked bark in it, let the fire ash ev...
Embodiment 3
[0050] A Dai cotton fire branding method. Set up raised parts of graphics or characters on the soldering iron, heat the soldering iron to 230 degrees, flatten the Dai cotton, and use the raised parts of the soldering iron to burn the Dai cotton for 1 second. Branded with graphics or text Dai cotton wrapping paper. The thickness of Dai cotton is 0.05mm.
[0051] The preparation method of the Dai cotton is:
[0052] (1) Material collection: in July and August every year, peel off the bark of the main trunk or branches of the mulberry tree with a knife, and then remove the green surface layer of the bark;
[0053] (2) drying material: hang the stripped bark inside and outside the yard, dry it and store it for later use;
[0054] (3) soaking: the dried bark is placed in water and soaked for 10 days;
[0055] (4) Ash mixing: first sieve the fire ash with a sieve to remove charcoal and other sundries, then place the soaked bark in it, let the fire ash evenly adhere to the bark, a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com