A method for preparing nanometer ferric oxide from water supply sludge
A technology of ferroferric oxide and water supply sludge, applied in the direction of iron oxide/hydroxide, nanotechnology for materials and surface science, nanotechnology, etc., can solve the problem that the iron salt coagulant components cannot be fully utilized, etc. problems, to avoid secondary pollution hazards, reduce production costs, and achieve the effect of recycling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0021] Specific embodiment one: this embodiment is a kind of method for preparing nano-ferric oxide ferric oxide with water supply sludge as raw material, specifically completes according to the following steps: 1. Preparation of water supply sludge powder: first, water supply sludge is naturally dried, Then grind to a particle size of less than 100 μm to obtain the water supply sludge powder; 2. Roasting: Put the water supply sludge powder into a box-type electric furnace, heat up from room temperature to 400-900 °C at a heating rate of 5 °C / min, and Roast at 400-900°C for 1 hour, then cool naturally to room temperature to obtain roasted feedwater sludge; 3. Acid leaching extraction: add the roasted feedwater sludge to acid at a solid-to-liquid ratio of 1:20, and stir at a stirring speed 400r / min and acid leaching temperature of 50-90°C for 1h-3h, then use a vacuum filter for vacuum filtration, then use distilled water as detergent, combined with vacuum filtration to wash the ...
specific Embodiment approach 2
[0025] Specific embodiment 2: The difference between this embodiment and specific embodiment 1 is that the water supply sludge described in step 1 is sludge from a sedimentation tank of a water purification plant. Others are the same as the first embodiment.
specific Embodiment approach 3
[0026] Embodiment 3: This embodiment differs from Embodiment 1 or Embodiment 2 in that the acid described in Step 3 is hydrochloric acid with a concentration of 2 mol / L. Others are the same as those in Embodiment 1 or 2.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com