A kind of bamboo plastic geothermal floor with negative ions and processing method thereof
A geothermal floor and negative ion technology, applied in the field of bamboo-plastic composite materials, can solve the problems such as the inability to meet the growing expansion of geothermal floors, no bamboo-plastic geothermal floors are found, poor dimensional stability, etc., achieving good market prospects, enhancing interface compatibility, The effect of good mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] A bamboo-plastic geothermal floor with negative ions is composed of the following components according to the mass ratio: 35% of bamboo powder, 25% of PVC and polyether block amide blend, 5% of nano-scale bamboo charcoal powder, 20% of germanium stone powder, lubricating 10% agent, 5% compatibilizer.
[0030] Among them, PVC and polyether block amide blends are mixed in a mass ratio of 8:2; the lubricant is a mixture of zinc stearate and ethylene bisstearic acid amide, mixed in a mass ratio of 6:4 into; coupling agent is silane coupling agent KH570.
Embodiment 2
[0032] A bamboo-plastic geothermal floor with negative ions is composed of the following components according to the mass ratio: 32% of bamboo powder, 28% of PVC and polyether block amide blend, 6% of nano-scale bamboo charcoal powder, 23% of germanium stone powder, lubricating Agent 8%, compatibilizer 3%.
[0033] Among them, PVC and polyether block amide blends are mixed in a mass ratio of 2:8; the lubricant is a mixture of zinc stearate and ethylene bisstearic acid amide, mixed in a mass ratio of 4:6 into; coupling agent is silane coupling agent KH570.
Embodiment 3
[0035] A bamboo-plastic geothermal floor with negative ions is composed of the following components according to the mass ratio: 25% of bamboo powder, 30% of PVC and polyether block amide blend, 7% of nano-scale bamboo charcoal powder, 25% of germanium stone powder, lubricating Agent 10%, coupling agent 3%.
[0036] Among them, PVC and polyether block amide blends are mixed at a mass ratio of 5:5; the lubricant is a mixture of zinc stearate and ethylene bisstearic acid amide, mixed at a mass ratio of 5:5. into; coupling agent is silane coupling agent KH570.
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 