A passivation process for nanomaterials
A nano-material and process technology, which is applied in the field of passivation process of nano-materials, can solve problems such as easy oxidation and loss of efficacy of bamboo charcoal powder, and achieve the effect of improving production efficiency and saving production time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Embodiment 1: A passivation process of nanomaterials, characterized in that: the passivation process includes the following steps:
[0016] A. Feeding: Put the nano bamboo charcoal powder to be passivated into the impact mill body, and then cover the lid to keep the impact mill body sealed;
[0017] B. Oxygen injection: Fill the impact mill with a proper amount of oxygen through the breathable one-way valve, so that the oxygen concentration in the impact mill is 250-280ppm, and the gas pressure in the impact mill is 0.12-0.13MPa. If the pressure is too high, the gas pressure The balance valve automatically deflates;
[0018] C. Passivation: Passivation of nano bamboo charcoal powder in the impact mill body, the passivation time is 14 hours, and the oxygen content is monitored in real time during passivation to keep the oxygen concentration in the impact mill body at 250-280ppm;
[0019] D. Deflate and stand: Open the gas release valve, release the gas in the impact mill, and le...
Embodiment 2
[0021] Embodiment 2: A passivation process of nano materials, characterized in that: the passivation process includes the following steps:
[0022] A. Feeding: Put the nano charcoal powder to be passivated into the impact mill body, and then cover the lid to keep the impact mill body sealed;
[0023] B. Oxygen injection: Fill the impact mill with a proper amount of oxygen through the breathable one-way valve, so that the oxygen concentration in the impact mill is 280-300ppm, and the gas pressure in the impact mill is 0.13-0.14MPa. If the pressure is too high, the gas pressure The balance valve automatically deflates;
[0024] C. Passivation: Passivation of nano charcoal powder in the impact mill, the passivation time is 18 hours, and the oxygen content is monitored in real time during passivation to keep the oxygen concentration in the impact mill at 280-300ppm;
[0025] D. Deflate and stand still: Open the gas release valve, release the gas in the impact mill, and let the passivated ...
PUM
Login to View More Abstract