A technology of cold and hot separation and water cups, which is applied to drinking utensils, household utensils, table utensils, etc., can solve the problems of poor anti-fall performance of the thermal insulation inner liner and easy breakage of the inner liner, and achieve easy replacement, destructive resistance, and good Effects of thermal insulation and impact resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] A method for preparing an impact-resistant thermos cup nanomaterial, comprising the following steps:
[0025] Step 1. Mix 26 parts of MOF-SO at room temperature 3 @SBA-15 nanomaterials, 39 parts of epoxy acrylic resin, 1.5 parts of methyl cellulose and 4 parts of talcum powder are added to a magnetic stirrer and mixed evenly at a speed of 500r / min, and then the processed mixture is put into a mold, and the The liquid is separated to obtain a shaped semi-wet mixture;
[0026] Step 2. Put the above-mentioned treated mixture and mold in a curing furnace for curing treatment. The curing temperature is 260°C and the holding time is 2 hours. After complete curing, it is cooled to room temperature with the furnace;
[0027] Step 3. The above-mentioned solidified material is subjected to stripping treatment, and then heated to 800°C in a muffle furnace for carbonization treatment. The holding time is 2 hours. After complete carbonization, it is cooled with the furnace;
[002...
Embodiment 2
[0035] Step 1. Mix 20 parts of MOF-SO at room temperature 3 @SBA-15 nanomaterials, 31 parts of epoxy acrylic resin, 1.5 parts of methyl cellulose and 4 parts of talcum powder are added to a magnetic stirrer and mixed evenly at a speed of 500r / min, and then the processed mixture is put into a mold, and the The liquid is separated to obtain a molded semi-wet mixture; other preparations are the same as in Example 1.
Embodiment 3
[0037] Step 1. Mix 16 parts of MOF-SO at room temperature 3 @SBA-15 nanomaterials, 49 parts of epoxy acrylic resin, 1.5 parts of methyl cellulose and 4 parts of talcum powder are added to a magnetic stirrer and mixed evenly at a speed of 500r / min, and then the processed mixture is put into a mold, and the The liquid is separated to obtain a molded semi-wet mixture; other preparations are the same as in Example 1.