Gravure printing craft

A gravure printing process, a technology of printing presses, applied in printing, post-processing of printing, printing devices, etc., can solve the problems of uneven inking, affecting printing quality, weak ink adhesion, etc.

Inactive Publication Date: 2018-05-18
重庆市金利药包材料有限公司
View PDF5 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

In the current gravure printing process, the ink adhesion is not strong and there is uneven ink deposition, which affects the quality of printing.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Gravure printing craft

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0023] This embodiment is basically as attached figure 1 Shown: a gravure printing process, including the following steps:

[0024] (1) Equip the printing machine: set the screen line and needle angle of the plate roller, install the plate roller on the printing machine in sequence according to the color sequence, and then install the embossing roller, doctor blade and ink fountain to complete the equipment of the printing machine;

[0025] (2) Ink preparation: The ink includes the following materials in parts by mass: 25 parts of alkyd resin, 4 parts of epoxy resin, 17 parts of ethanol, 22 parts of isopropanol, 4 parts of wax slurry, 1 part of surfactant, acetyl lemon 3 parts of tributyl ester, 6 parts of triethanolamine, 2 parts of fungicide;

[0026] (3) Proofing: install the proofing film on the reel, clamp the end, fix the film roll, and wear the proofing film according to the route specified by the printing machine, and wind the film head on the installed winding mandre...

Embodiment 2

[0034] The difference between this embodiment and the embodiment is that step (2) ink preparation includes the following materials in parts by mass: 20 parts of alkyd resin, 3 parts of epoxy resin, 15 parts of ethanol, 18 parts of isopropanol, 3 parts of wax slurry 1 part, 1 part of surfactant, 1 part of acetyl tributyl citrate, 5 parts of triethanolamine, 1 part of fungicide. When the printing speed is 100-140m / min, the drying temperature in step (7) changes with the change of the graphic area, specifically when the graphic area is 0-20%, the drying temperature is 30-50°C, when The graphic area is 30-70%, and the drying temperature is 50-70°C. When the graphic area is 80-100%, the drying temperature is 60-80°C. The printing film is easily softened by heat and elongates under the action of tension. Therefore, the inventors have found through many tests that for different printing speeds and different image and text areas, the effect of using the above drying temperature is bet...

Embodiment 3

[0036] The difference between this embodiment and the embodiment is that step (2) ink preparation includes the following materials in parts by mass: 30 parts of alkyd resin, 5 parts of epoxy resin, 20 parts of ethanol, 25 parts of isopropanol, 5 parts of wax slurry 2 parts, 2 parts of surfactant, 5 parts of acetyl tributyl citrate, 8 parts of triethanolamine, 3 parts of fungicide. Further, when the printing speed is 140-160m / min, the drying temperature in step (7) changes with the area of ​​the image and text, specifically when the area of ​​the image and text is 0-20%, the drying temperature is 30-50°C , when the graphic area is 30-70%, the drying temperature is 50-70°C, when the graphic area is 80-100%, the drying temperature is 65-85°C. The printing film is easily softened by heat and elongated under the action of tension. Therefore, the inventors have found through many tests that for different printing speeds and different image and text areas, the above drying temperatur...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention belongs to the field of printing, and particularly discloses a gravure printing craft. The gravure printing craft includes the following steps that (1), equipping of a printing device, (2), preparation of printing ink, (3), making of a proof, (4), electric corona, (5), pretreatment of a printing plate, (6), printing, and (7), drying, specifically, a printing film is dried. The gravure printing craft can improve the gravure printing quality.

Description

technical field [0001] The invention relates to the technical field of printing, in particular to a gravure printing process. Background technique [0002] Gravure printing is a plate-making technique in which an image is engraved from a surface in depressions. Generally speaking, copper or zinc plate is used as the engraved surface, and the concave part can be etched, engraved, copper engraving or metal plate making method. To print a gravure plate, the surface is covered with ink, which is then wiped from the surface with tartham or newspaper, leaving only the depressions. Wet paper is placed on top of the printing plate, and the printing plate and paper are pressed through the printing press, which transfers the ink from the recessed part of the printing plate to the paper. The current gravure printing process has weak ink adhesion and uneven ink deposition, which affects the quality of printing. Contents of the invention [0003] The object of the present invention ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): B41M1/10B41M5/00B41M7/00C09D11/105C09D11/102C09D11/12C09D11/03
CPCB41M1/10B41M5/0011B41M7/009C09D11/03C09D11/102C09D11/105C09D11/12
Inventor 毛泽容
Owner 重庆市金利药包材料有限公司