Colored asphalt with high performance
A high-performance technology of colored asphalt, which is applied in the field of road engineering, can solve the problems that the performance of colored asphalt needs to be improved, and achieve the effect of improving vision and beautifying the environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A high-performance colored asphalt, which is made of the following parts by weight of raw materials: 52 parts by weight of epoxy resin, 24 parts of petroleum resin, 5 parts of styrene-butadiene-styrene block copolymer, and furfural extractable oil 38 parts, 3 parts of dioctyl phthalate, 6 parts of diatomaceous earth, 9 parts of inorganic pigments.
[0016] Among them, the inorganic pigment is iron red pigment.
[0017] The preparation method includes the following steps: heating the furfural extraction oil to 160-180°C, then adding petroleum resin, epoxy resin, and styrene-butadiene-styrene block copolymer to stir, and then cooling to 120-140°C, Then add dioctyl phthalate and diatomaceous earth and stir, and finally add inorganic pigments and stir to get the product.
Embodiment 2
[0019] A high-performance colored asphalt, which is made of the following parts by weight of raw materials: 55 parts by weight of epoxy resin, 25 parts of petroleum resin, 8 parts of styrene-butadiene-styrene block copolymer, and furfural extractable oil 40 parts, 5 parts of dioctyl phthalate, 8 parts of diatomaceous earth, 12 parts of inorganic pigments.
[0020] Among them, the inorganic pigment is a chrome yellow pigment.
[0021] The preparation method includes the following steps: heating the furfural extraction oil to 160-180°C, then adding petroleum resin, epoxy resin, and styrene-butadiene-styrene block copolymer to stir, and then cooling to 120-140°C, Then add dioctyl phthalate and diatomaceous earth and stir, and finally add inorganic pigments and stir to get the product.
Embodiment 3
[0023] A high-performance colored asphalt, which is made of the following parts by weight of raw materials: 55 parts by weight of epoxy resin, 25 parts of petroleum resin, 8 parts of styrene-butadiene-styrene block copolymer, and furfural extractable oil 40 parts, 5 parts of dioctyl phthalate, 8 parts of diatomaceous earth, 12 parts of inorganic pigments.
[0024] Among them, the inorganic pigment is iron green pigment.
[0025] The preparation method includes the following steps: heating the furfural extraction oil to 160-180°C, then adding petroleum resin, epoxy resin, and styrene-butadiene-styrene block copolymer to stir, and then cooling to 120-140°C, Then add dioctyl phthalate and diatomaceous earth and stir, and finally add inorganic pigments and stir to get the product.