The processing technology of Tan sheepskin, Tan sheepskin and fur products
A treatment process and sheepskin technology, applied in fur mechanical treatment, small raw hide/big raw hide/leather/fur treatment, small raw hide/large raw hide/leather/fur mechanical treatment, etc. Fur products are of low grade and the added value of Tan sheep second fur cannot be improved, so as to achieve the effect of smooth and uniform fur ears, good retention, and avoid hard and brittle fur
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0054] A treatment process for beach wool skin, comprising:
[0055] S1. Tanning the Tan sheepskin after the pre-tanning treatment, specifically including:
[0056] Control the water temperature at 36°C, stir the Tan sheepskin sheets in the white tanning solution with a white tanning agent concentration of 3.0g / L, a formic acid concentration of 1.5g / L, and a salt concentration of 50g / L for about 30 minutes, then turn it off and combine it overnight, turn it off When combined, it rotates for about 5 minutes per hour and then stops. Add baking soda according to the standard of 2.0 per liter of solution, stir for about 30 minutes, turn and stop for about 4 hours, and turn and stop for about 5 minutes per hour and then stop. Add soda ash in 5-6 times until the pH stabilizes to 7.8-8.0, and let stand overnight.
[0057] S2. Neutralizing and retanning the Tan sheepskin, specifically including:
[0058] The water temperature was controlled at 38°C, and Tan sheepskins were treated ...
Embodiment 2
[0066] A kind of processing technology of beach sheepskin, its difference with embodiment 1 is: in the S3 step, the beach sheepskin sheet adopts machine comb uniformly. The operation of all the other S1, S2, S4 is identical with embodiment 1.
[0067] After testing, the obtained beach wool fur: the leather board is soft and severely damaged. Skin board shrinkage temperature ≥85°C. The nine curves of the hair ears are not obvious, the hair ears are uneven, and the coat color is smooth. Detected formaldehyde content ≤ 75mg / kg.
[0068] The shrinkage temperature of the tanned sheepskin is high, no chrome tanning is required before dyeing, and hexavalent chromium is not detected in the dyed product.
Embodiment 3
[0070] A kind of treatment process of beach sheepskin, its difference with embodiment 1 is: in S4 step, adopt common water to carry out water shedding as hanging washing liquid. The operation of all the other S1, S2, S3 is the same as in Embodiment 1.
[0071] After testing, the obtained beach wool fur is soft and has good integrity. Skin board shrinkage temperature ≥85°C. The nine curves of the hair ears are more obvious, the hair ears are uneven, and the coat color is not smooth. Detected formaldehyde content ≤ 75mg / kg.
[0072] The shrinkage temperature of the tanned sheepskin is high, no chrome tanning is required before dyeing, and hexavalent chromium is not detected in the dyed product.
PUM
Property | Measurement | Unit |
---|---|---|
temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com