A kind of preparation method of vanadium-doped antibacterial papermaking material
A technology of antibacterial materials and technical solutions, which is applied in the field of preparation of vanadium-doped antibacterial paper-making materials, and can solve problems such as easy detachment or dissolution, and user health hazards
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A method for preparing a vanadium-doped antibacterial paper-making material, the preparation technical scheme is as follows:
[0020] According to the number of parts by mass, 10 parts of straw, 12 parts of straw, 18 parts of bagasse, 4 parts of carboxymethyl cellulose and 60 parts of water are added to a beater for beating and stirring to form a slurry, and then heated to 95 ° C. Keep warm for 3 hours to separate the fibers in the oar liquid, add 40 parts of thermoplastic starch to the system, stir for 20 minutes, then add 3 parts of fermentation enzyme, stir evenly, control the temperature at 40°C, and ferment for 20 hours; after the fermentation is completed, wash the precipitate, Then add 5 parts of vanadium-doped antibacterial materials and 8 parts of fillers to condense the raw materials, then dehydrate to form a paste, then add 3 parts of defoamer and 5 parts of whitening agent and stir evenly, continue beating for 20 minutes, and then add 8 parts of sizing agent...
Embodiment 2
[0029] A method for preparing a vanadium-doped antibacterial paper-making material, the preparation technical scheme is as follows:
[0030] According to the number of parts by mass, 5 parts of straw, 10 parts of straw, 12 parts of bagasse, 2 parts of carboxymethyl cellulose and 50 parts of water are added to a beater for beating and stirring to form a slurry, and then heated to 90°C. Insulate for 1 hour to separate the fibers in the oar liquid, add 30 parts of thermoplastic starch to the system, stir for 10 minutes, then add 1 part of fermentation enzyme, stir evenly, control the temperature at 30°C, and ferment for 10 hours; after the fermentation is completed, wash the precipitate, Then add 1 part of vanadium-doped antibacterial material and 5 parts of filler to condense the raw materials, then dehydrate to form a paste, then add 1 part of defoamer and 3 parts of whitening agent and stir evenly, continue beating for 10 minutes, and then add 5 parts of sizing agent, stirred ...
Embodiment 3
[0039] A method for preparing a vanadium-doped antibacterial paper-making material, the preparation technical scheme is as follows:
[0040] According to the number of parts by mass, 20 parts of straw, 14 parts of straw, 28 parts of bagasse, 8 parts of carboxymethyl cellulose and 80 parts of water are added to a beater for beating and stirring to form a slurry, and then heated to 105 ° C. Keep warm for 5 hours to separate the fibers in the oar liquid, add 50 parts of thermoplastic starch to the system, stir for 30 minutes, then add 5 parts of fermentation enzyme, stir evenly, control the temperature at 50°C, and ferment for 40 hours; after the fermentation is completed, wash the precipitate, Then add 10 parts of vanadium-doped antibacterial materials and 10 parts of fillers to condense the raw materials, then dehydrate to form a paste, then add 5 parts of defoamers and 8 parts of whitening agents and stir evenly, continue beating for 30 minutes, and then add 10 parts of sizing...