A manufacturing method and optical fiber technology, which is applied in the field of manufacturing intermittently fixed cored wires, can solve the problems of increased optical transmission loss, increased optical fiber transmission speed, and unstable range of joint formation, so as to improve manufacturing efficiency and stabilize the range Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] In this example, studies were conducted to confirm the advantages of the above-described manufacturing method.
[0035] Specifically, after the optical fibers 1 are collectively coated as described above, the transport speed V1 at the time of transporting them to the rotary blade 21 is changed. The peripheral velocity V2 is set constant. Then, as the intermittently fixed core wire 10 of Example 1, an intermittently fixed core wire in which the coating material 2 was partially cut off by the rotary blade 21 to form the connecting portion 2 a was produced.
[0036] In addition, in Example 1, as the optical fiber 1, the colored fiber optic core wire. In addition, the number of optical fibers 1 included in the intermittent fixed tape core wire 10 was set to twelve. The conveyance speed V1 of the optical fiber 1 to be coated together is varied in the range of 200 to 1200 (m / min).
[0037]Furthermore, in order to compare with this Example 1, the uncured resin which will ...
Embodiment 2
[0044] In the present embodiment, studies concerning the ratio of the conveying speed V1 to the peripheral speed V2 of the rotary knife 21 were conducted.
[0045] Specifically, as fiber 1 used the After coating 12 of the colored optical fiber core wires, the coating material 2 was partially cut with the rotary knife 21 to form the connecting portion 2a. At this time, the ratio of the conveyance speed V1 to the peripheral speed V2 is changed. Moreover, when changing this ratio, if the same rotary blade 21 is used, the length of the connection part 2a and the separation part 2b in the longitudinal direction X will change. Therefore, in this embodiment, the number of notches 21b provided in the rotary blade 21 is changed by changing the ratio of the conveying speed V1 to the peripheral speed V2, and the lengths of the connecting portion 2a and the separating portion 2b are adjusted to be constant. . For example, when V1:V2=4:1, the rotary blade 21 with eight notches 21b is u...
Embodiment 3
[0054] In the present embodiment, the preferred shape of the rotary blade 21 was studied.
[0055] Specifically, prepared to change image 3 The various types of rotary blades 21 having the ratios of b1 and n1 shown above were used to produce the intermittent fixed tape core wire 10 . The position and number of the cutouts 21b of the above-mentioned rotary blade 21 and image 3 Same as shown. That is, the rotary blade 21 provided with a pair of notch part 21b in the radially opposing position across the central axis O is used. Each of the rotary blades 21 has a point-symmetrical shape with respect to the central axis O. As shown in FIG. Therefore, n1=n2, b1=b2. In addition, n1:b1=n2:b2=N:B. The ratio of n1 to b1 (that is, the ratio of the length N of the connection portion to the length B of the cut portion) is changed within the range of 3:1 to 1:25.
[0056] In addition, in this example using The colored optical fiber core wires of the above-mentioned colored optical...