Processing method of improved low VOC volatilized cowhide sofa leather
A processing method and technology for sofa leather, which can be used in leather drying, leather manufacturing, special leather manufacturing, etc., and can solve the problems of heavy product odor, high total carbon emission, and non-compliance with environmental protection requirements.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0069] The following are specific embodiments of the present invention and in conjunction with the accompanying drawings, the technical solutions of the present invention are further described, but the present invention is not limited to these embodiments.
[0070] The processing method of the volatilized cowhide sofa leather of this improved type low VOC comprises the following steps:
[0071] a, depilation: the rawhide is depilated one by one by a hair pushing machine; in the present embodiment, the hair pushing machine adopts existing equipment available on the market;
[0072] b, softening: the raw hide after depilation is softened under the action of softening enzyme, the amount of softening enzyme is 1-2% of the weight of raw hide, the softening temperature is 28-34 ° C, and the softening time is 20-30min; in this embodiment , softening the rawhide after depilation under the action of softening enzyme, the amount of softening enzyme is 1.5% of the weight of the hide, the...
PUM
| Property | Measurement | Unit |
|---|---|---|
| softening point | aaaaa | aaaaa |
| water content | aaaaa | aaaaa |
Abstract