Artemisinin silver ion composite disinfectant
A technology of artemisinin and silver ions, which is applied in the direction of disinfectants, biocides, animal repellents, etc., can solve the problems of practical value discount, explosion, and inability to spray disinfection, and achieve the effect of preventing occurrence and spread
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation Embodiment 1
[0013] Preparation Example 1: The preparation method of a kind of artemisinin silver ion composite disinfectant of the present invention specifically comprises the following steps:
[0014] 1. The preparation of the silver ion complex, first take 76% of alkyl glycoside citrate and 11% of phosphoric acid, fully fused to prepare a complexing agent, then add a total of 4% of silver nitrate, and the rest are all deionized Water, the sum of the above components is 100%, put the above mixture into a reaction kettle with a stirring head and an emulsifying head, fully stir and react for 22 minutes to make a silver ion complex, and then stand at room temperature 25 hours;
[0015] 2. Prepare the raw materials according to the following weight: take 22g artemisinin, 49.9g 50% hydrogen peroxide, 28g glacial acetic acid, add them to the reaction kettle with stirring head and emulsifying head, and then add the prepared silver ion of 0.1g Complex compound, the sum of the above components i...
preparation Embodiment 2
[0017] Preparation Example 2: The preparation method of a kind of artemisinin silver ion composite disinfectant of the present invention specifically comprises the following steps:
[0018] 1. The preparation of silver ion complex, first take 78% of alkyl glycoside citrate and 13% of phosphoric acid, fully fused to prepare a complexing agent, then add a total of 5% of silver nitrate, and the rest are all deionized Water, the sum of the above components is 100%, put the above mixture into a reaction kettle with a stirring head and an emulsifying head, fully stir and react for 28 minutes to make a silver ion complex, and then stand at room temperature 28 hours;
[0019] 2. Prepare the raw materials according to the following weight: take 24g of artemisinin, 48.85g of 50% hydrogen peroxide, and 27g of glacial acetic acid, add them to the reaction kettle with a stirring head and an emulsifying head, and then add 0.15g of prepared silver ions Complex compound, the sum of the above...
preparation Embodiment 3
[0021] Preparation Example 3: The preparation method of a kind of artemisinin silver ion composite disinfectant of the present invention specifically comprises the following steps:
[0022] 1. The preparation of the silver ion complex, first take 77% of alkyl glycoside citrate and 14% of phosphoric acid, fully fused to prepare a complexing agent, then add a total of 6% of silver nitrate, and the rest are all deionized Water, the sum of the above components is 100%, put the above mixture into a reaction kettle with a stirring head and an emulsifying head, fully stir and react for 20-30 minutes to make a silver ion complex, and then, at room temperature Stand for 34 hours;
[0023] 2. Prepare the raw materials according to the following weight: take 25g of artemisinin, 48.8g of 50% hydrogen peroxide, and 26g of glacial acetic acid, add them to the reaction kettle with a stirring head and an emulsifying head, and then add 0.20g of prepared silver ions Complex, the sum of the abo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap