Copybook and manufacturing method thereof
A production method and technology for copybooks, applied in the field of copy copybooks, can solve the problems of inability to accurately judge the defects and deviations of writing fonts, poor calligraphy effect, and long time consumption, so as to avoid writing habits and achieve good calligraphy effect. , the effect of good use value
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0055] The purpose of this embodiment is to provide a kind of copybook, and its manufacturing process is specifically as follows:
[0056] Coat one side of the PET transparent substrate with a water-based coating solution with a viscosity of 65pa·s, and then cure it by heating and compounding ultraviolet rays. The heating temperature is 95°C, and the light intensity of ultraviolet rays is 8.5kW / cm 2 . After the ink-absorbing layer is solidified, print reference characters on it, and dry it for 45 minutes at a temperature of 165° C. to obtain a copybook.
Embodiment 2
[0058] The purpose of this embodiment is to provide a kind of copybook, and its manufacturing process is specifically as follows:
[0059] An adhesive layer was coated on one side of the PET transparent substrate, and dried at 80° C. for 2 hours. Then apply a water-based coating solution on one side of the adhesive layer, the viscosity of which is 55pa·s, and then cure by heating and compounding ultraviolet rays. The heating temperature is 80°C, and the light intensity of ultraviolet rays is 7kW / cm 2 . After the ink-absorbing layer is solidified, print reference characters on it, and dry it for 60 minutes at a temperature of 150° C. to obtain a copybook.
Embodiment 3
[0061] The purpose of this embodiment is to provide a kind of copybook, and its manufacturing process is specifically as follows:
[0062] An adhesive layer was coated on one side of the PET transparent substrate, and dried at 110° C. for 4 hours. Then apply a water-based coating liquid on one side of the adhesive layer, the viscosity of which is 75pa·s, and then cure by heating and compounding ultraviolet rays. The heating temperature is 110°C, and the light intensity of ultraviolet rays is 10kW / cm 2 . After the ink-absorbing layer is cured, print reference characters on it, and dry it at 180°C for 30 minutes, then coat it with a transparent layer of varnish, and dry it at 120°C for 2 minutes , make a copybook.