Wadding of mineral toy
A technology for fillers and toys, used in toys, dolls, entertainment, etc., can solve the problems of high iron content, dark particles, and difficulty in promotion.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0019] Below in conjunction with embodiment, the present invention will be further described:
[0020] 1. The ingredients of the mineral toy filler include the following components by weight percentage: attapulgite clay powder 54%, white cement 18%, expanded perlite powder 14%, expanded vermiculite powder 10% and titanium dioxide 4%.
[0021] 2. The preparation method of the mineral toy filling material is: use a mixer to mix the ingredients of the mineral toy filling material evenly, and transport them to the granulator for granulation. The particle size is controlled at 4.0 mm. After granulation, transport them to the indoor ground Ping is dried, and the drying time is controlled within 5 days. When the water content of the granules is less than 15%, it is dried at a low temperature. The temperature is controlled at 100 ° C, and the drying time is controlled within 5 hours. After cooling, the water content of the granules is less than 2%. Packaged as a finished product.