Water-base chain lubricating agent
A technology for lubricants and chains, applied in lubricating compositions, petroleum industry, etc., can solve the problems of high solid content, poor resistance to hard water, scale blockage of sprinklers, etc., to improve the workshop environment, prolong service life, reduce The effect of pour rate
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Publication Date
- 2010-12-08
Abstract
Description
Technical field
[0001] The invention relates to a lubricant used in high-speed conveyor belt production lines such as PET bottles, glass bottles and cans, and belongs to the field of chemical lubricants.
Background technique
[0002] Lubricants for the lubrication system of the filling line have experienced more than 40 years of development. In the original semi-automatic filling system, the bottle conveying speed of the production line was only a few hundred bottles to one thousand bottles per hour. The bottle conveying system did not have a special lubricant, and the bottle and the chain were in a state of dry friction, so the wear of the chain was serious. Later, people noticed this problem and installed a soap soaking tank for the bottle conveying system to lubricate the chain with soap, which solved the problem of chain wear to a certain extent. But this type of lubricant has the following disadvantages: (1) poor solubility, easy hydrolysis, and poor resistance to ...
Examples
Embodiment 1
[0047] (1) Mix 50g triethanolamine oleate and 60g triethanolamine, stir well, add 60g gluconoside and stir for 15 minutes, then add 30g LF-131, 20g isothiazolinone, 10g polymaleic acid, 10g benzene Piantriazole, 10g sodium xylene sulfonate were stirred for 30 minutes;
[0048] (2) Add 50g of EDTA-2Na into 700g of pure water, heat to 50°C and stir until it dissolves evenly;
[0049] (3) Mix the mixture obtained in the above two steps and stir evenly.
[0050] (4) Sealed and protected from light, diluted with industrial water at a ratio of 1:200 and sprayed for use.
Embodiment 2
[0052] (1) Mix 20g triethanolamine oleate and 30g triethanolamine, stir well, add 40g gluconoside and stir for 15 minutes, then add 10g LF-131, 10g isothiazolinone, 10g polymaleic acid, 10g benzene Piantriazole, 10g sodium xylene sulfonate were stirred for 30 minutes;
[0053] (2) Add 30g of EDTA-2Na into 650g of pure water, heat to 53°C and stir until it dissolves evenly;
[0054] (3) Mix the mixture obtained in the above two steps and stir evenly.
[0055] (4) Sealed and protected from light, diluted with industrial water at a ratio of 1:200 and sprayed for use.
Embodiment 3
[0057] (1) Mix 70g triethanolamine oleate and 90g triethanolamine, stir evenly, add 70g gluconoside and stir for 15 minutes, then add 30g LF-131, 20g isothiazolinone, 20g polymaleic acid, 20g benzene Piantriazole, 20g sodium xylene sulfonate were stirred for 30 minutes;
[0058] (2) Add 60g of EDTA-2Na into 750g of pure water, heat to 60°C and stir until it dissolves evenly;
[0059] (3) Mix the mixture obtained in the above two steps and stir evenly.
[0060](4) Sealed and protected from light, diluted with industrial water at a ratio of 1:200 and sprayed for use.