A rapid determination, stone coal mine technology, applied in the direction of chemical analysis by titration, preparation of test samples, analysis by chemical indicators, etc., can solve the problems of time-consuming, difficult to decompose, affect the judgment of color, etc., to achieve color The effect of clear judgment, simple operation and large sampling volume
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] Embodiment 1 will be taken from the stone coal mine (recorded as 1#) of a certain place in Hunan to carry out the mensuration of vanadium:
[0022] (1) Ore sample pretreatment and ore sample dissolution: the stone coal ore was crushed and finely ground until its particle size passed through a 200-mesh sieve, and then dried in an oven at 105°C for 2 hours. Take 5g of the dried ore sample in a plastic cup, gradually add 2mL of analytically pure hydrofluoric acid, and after leaching for 1 hour at room temperature, move all the ore pulp into a beaker, add 4mL of sulfuric acid (1+1), and leaching for 3 hours at 95°C. , filtered and washed while hot, and the volume of the filtrate was constant to 100mL;
[0023] (2) Drugs and reagents:
[0024] Sulfuric acid (analytical pure);
[0025] Sulfuric acid (1+1): prepared by mixing 1 volume of sulfuric acid with 1 volume of water;
[0026] Sulfuric acid (5+95): prepared by mixing 5 volumes of sulfuric acid with 95 volumes of wate...
Embodiment 2
[0046] Embodiment 2 (the preparation of medicine and reagent is the same as embodiment 1)
[0047] The stone coal mine (denoted as 2#) taken from a certain place in Guizhou was crushed and finely ground until its particle size passed through a 200-mesh sieve. It was dried in an oven at 105°C for 3 hours, and 10 g of the ore sample was taken in a plastic cup. Gradually add 4mL of analytically pure hydrofluoric acid, stir and leach for 2h at room temperature, add 5mL of sulfuric acid (1+1), and leach for 4h at 95°C, filter and wash while hot, and make the volume of the filtrate to 100mL. Take 1mL of the filtrate into a 300mL Erlenmeyer flask, and rinse the inner wall of the bottle with a small amount of water. Add 20mL of sulfuric acid (1+1), 5mL of phosphoric acid (1+1), dilute with water to about 100mL, place to cool, add 5mL of ferrous sulfate, wait for 2min, add potassium permanganate dropwise under artificial shaking conditions until the solution turns red , wait for 5 min...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com