Method for producing optical display device and winding-up roller for producing optical display device
A technology of optical display and manufacturing method, which is applied in the direction of chemical instruments and methods, optics, lamination devices, etc., can solve the problems of easy peeling at the end, and achieve the effects of preventing peeling, preventing the mixing of air bubbles, and preventing scratches
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0082] In Example 1, a single-sided protective polarizing plate with a polarizer protective film attached to only one side of the polarizing film was cut out from a roll formed by rolling one side of the release film inside. The polarizing plate was bonded to the optical display unit while applying a tension of 50 N / m. The amount of warping toward the release film side of the polarizing plate when cut out was 80 mm. In this Example 1, the variation in the bonding position was as small as ±1 mm or so. In addition, regarding the peeling of the end face, peeling was not confirmed under any circumstances.
Embodiment 2
[0084] In Example 2, a single-sided protective polarizing plate with a polarizer protective film bonded to only one side of the polarizing film was cut out from a roll formed by rolling one side of the release film inside. The polarizing plate was bonded to the optical display unit while applying a tension of 350 N / m. The amount of warping toward the release film side of the polarizing plate when cut out was 80 mm. In this Example 2, the variation in the bonding position was as small as about ±1 mm. In addition, regarding the peeling of the end face, peeling was not confirmed under any circumstances.
Embodiment 3
[0086] In Example 3, a single-sided protective polarizing plate with a polarizer protective film attached to only one side of the polarizing film was cut out from a roll formed by rolling one side of the release film inside. The polarizing plate was bonded to the optical display unit while applying a tension of 500 N / m. The amount of warping toward the release film side of the polarizing plate when cut out was 80 mm. In Example 3, the variation in the bonding position was as small as about ±1 mm. In addition, regarding the peeling of the end face, peeling was not confirmed under any circumstances.
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 