A kind of drying method of lithium-ion battery cell
A lithium-ion battery and drying method technology, which is applied in drying solid materials, electrolyte battery manufacturing, non-aqueous electrolyte battery and other directions, can solve problems such as long drying time, air permeability change, battery deformation, etc., to reduce labor load and simplify operation. effect of the process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] An ultra-thick battery cell 904586 wound by cathode, anode, and diaphragm, put it into a packaging case, seal on three sides, and leave one side open for drying water and filling electrolyte. This batch of batteries to be packaged The core is placed in a drying oven (that is, placed in a closed cavity), and the drying oven can realize a cavity with a vacuum degree greater than 98% and a temperature greater than or equal to 120°C. , The gas in the drying furnace is dry air. First, the furnace cavity of the drying furnace is heated up to 60°C, and the temperature is kept constant. Apply the drying method of the present invention to vacuumize and detect the vacuum degree in the furnace. When the vacuum degree is less than -96KPa, delay the timer and keep it for 15 minutes. Unload the vacuum, then delay for 1 minute, repeat the above vacuuming and vacuuming actions, form a circulating gas flow in the drying furnace, cycle 20 times, then enter the vacuum drying stage, vacuum...
Embodiment 2
[0023] The difference from Example 1 is that the drying gas filled in the drying furnace is nitrogen, the constant temperature is 100°C, the delay treatment time is 10 minutes, and the cycle is 22 times. After entering the vacuum drying stage, keep it for 200 minutes. The drying time is 7 hours. Summarizing the water content test results of 15 batches, the average water content is 110.1ppm.
Embodiment 3
[0025] The difference from Example 1 is that the constant temperature is 30°C, the delayed treatment time is 5 minutes, and the cycle is 50 times. After entering the vacuum drying stage, it is kept for 410 minutes. The drying time of the process is 11 hours, and 15 batches of water are summarized. As a result of the content test, the average water content is 128.3ppm.
PUM
Property | Measurement | Unit |
---|---|---|
thermal resistance | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com