Method for the quantitative measurement of the mechanical stability time (mst) of latex suspensions and equipment used in said method
A technology of mechanical stability and quantitative measurement, applied in the direction of measuring devices, flow characteristics, instruments, etc., can solve time-consuming problems, achieve the effect of enhancing accuracy and reducing test duration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0062] Preparation of Latex Suspension Test Samples
[0063] Preparation of latex suspension test samples depends on the particular type of suspension to be tested. Generally, methods for sample preparation for qualitative testing of such suspensions are specified in ISO and ASTM standards.
[0064] For example, as previously mentioned, the standard tests for MST determination of natural rubber latex are those specified in tests ISO35 and ASTM D-1076. These standards all state that the latex (concentrate) is first diluted with ammonia to a total solids content of approximately 55% and subsequently heated to a temperature between approximately 36°C and 37°C. The diluted and heated latex sample is then preferably filtered through a stainless steel strainer prior to testing.
[0065] Standard tests for the determination of the MST of synthetic rubbers are specified in ISO2006 and ASTM D1417-90.
[0066] stir suspension
[0067] The stirrer 10 is arranged to be immersed in...
PUM
| Property | Measurement | Unit |
|---|---|---|
| diameter | aaaaa | aaaaa |
| force | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 