A glass panel and mobile phone technology, applied in printing, printing devices, etc., can solve the problems of low product yield, poor light-shielding performance, poor adhesion ability, etc., achieve excellent adhesion performance, enhance the light-shielding effect, and improve the light-shielding effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0043] A printing process for a glass panel of a mobile phone is to perform multiple bottom cover printing on the back of the glass panel, which specifically includes the following steps:
[0044] Step 1. The first white background printing: the first white background printing layer is printed on the back of the glass panel of the mobile phone by screen printing. The printing materials required by weight are: 100 parts of ink, 9 parts of curing agent and thinner 4 copies, the screen mesh number of the screen printing is 400 meshes, the hardness of the squeegee board is 75A, the curing temperature is 145°C, the curing time is 35 minutes, and the overall thickness of the ink after printing is 6μm.
[0045] Step 2. The second white background printing: the second white background printing layer is printed on the first white background printing layer. The printing materials required by weight are: 100 parts of ink, 8 parts of curing agent and 3 parts of diluent , The screen mesh of the...
Embodiment 2
[0049] A printing process for a glass panel of a mobile phone is to perform multiple bottom cover printing on the back of the glass panel, which specifically includes the following steps:
[0050] Step 1. The first white background printing: the first white background printing layer is printed on the back of the glass panel of the mobile phone by screen printing. The printing materials required by weight are: 100 parts of ink, 8 parts of curing agent and thinner 3 copies, the screen mesh number of the screen printing is 420, the hardness of the squeegee board is 80A, the curing temperature is 140°C, the curing time is 40 minutes, and the overall thickness of the ink after printing is 7μm.
[0051] Step 2. The second white background printing: the second white background printing layer is printed on the first white background printing layer. The printing materials required by weight are: 100 parts of ink, 9 parts of curing agent and 4 parts of diluent , The screen mesh of the screen...
Embodiment 3
[0055] A printing process for a glass panel of a mobile phone is to perform multiple bottom cover printing on the back of the glass panel, which specifically includes the following steps:
[0056] Step 1. The first white background printing: the first white background printing layer is printed on the back of the glass panel by screen printing. The materials required for printing are: 100 parts of ink, 10 parts of curing agent and 4 parts by weight. The screen printing screen mesh is 450 meshes, the hardness of the squeegee is 70A, the curing temperature is 150°C, the curing time is 25 minutes, and the thickness of the printing ink is 7μm.
[0057] Step 2. The second white background printing: the second white background printing layer is printed on the first white background printing layer. The materials required for printing are: 100 parts of ink, 10 parts of curing agent and 4 parts by weight. The screen printing screen mesh number is 370 meshes, the hardness of the squeegee is 8...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com