a luminous paint
A paint and luminescent powder technology, applied in the field of paint, can solve the problem that paint cannot produce marks, and achieve the effect of reducing maintenance costs and saving electric energy
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A luminous paint of this embodiment, the parts by weight of its components are: 10 parts of acrylate, 4 parts of epoxy resin, 3 parts of polyvinyl chloride resin, 12 parts of water, 5 parts of luminescent powder, 3 parts of alkyd resin 12 parts, 12 parts of acrylonitrile, 4 parts of phthalic anhydride, 11 parts of tung oil, 1 part of zinc phosphate, 2 parts of basic lead silicochromate, 5 parts of thinner, and 2 parts of drier.
[0013] The luminescent powder is made of strontium aluminosilicate or alkaline earth metal aluminate.
[0014] The thinner material is formed by mixing white beet oil, white alcohol, and white alcohol in a ratio of 1:3:1.
[0015] The drier uses cobalt drier and is used in conjunction with manganese, zirconium, lead, zinc and calcium drier.
Embodiment 2
[0017] A luminous paint of this embodiment, the parts by weight of its components are: 13 parts of acrylate, 7 parts of epoxy resin, 6 parts of polyvinyl chloride resin, 15 parts of water, 8 parts of luminescent powder, 6 parts of alkyd resin 15 parts of acrylonitrile, 6 parts of phthalic anhydride, 16 parts of tung oil, 4 parts of zinc phosphate, 4 parts of basic lead silicochromate, 8 parts of thinner, and 2 to 7 parts of drier.
[0018] The luminescent powder is made of strontium aluminosilicate or alkaline earth metal aluminate.
[0019] The thinner material is formed by mixing white beet oil, white alcohol, and white alcohol in a ratio of 1:3:1.
[0020] The drier uses cobalt drier and is used in conjunction with manganese, zirconium, lead, zinc and calcium drier.
Embodiment 3
[0022] A luminous paint of this embodiment, the parts by weight of its components are: 11 parts of acrylate, 6 parts of epoxy resin, 4 parts of polyvinyl chloride resin, 13 parts of water, 7 parts of luminous powder, 4 parts of alkyd resin 13 parts, 13 parts of acrylonitrile, 5 parts of phthalic anhydride, 14 parts of tung oil, 3 parts of zinc phosphate, 3 parts of basic lead silicochromate, 6 parts of thinner, and 4 parts of drier.
[0023] The luminescent powder is made of strontium aluminosilicate or alkaline earth metal aluminate.
[0024] The thinner material is formed by mixing white beet oil, white alcohol, and white alcohol in a ratio of 1:3:1.
[0025] The drier uses cobalt drier and is used in conjunction with manganese, zirconium, lead, zinc and calcium drier.