A topcoat, water-based technology, used in polyurea/polyurethane coatings, coatings, etc., can solve the problems of paint pollution and poor thermal insulation performance, and achieve improved thermal insulation performance, good thermal insulation performance, and good reflective performance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] (1) Weigh 250g of glass beads, 226g of deionized water, 100g of filler and 60g of additives and stir evenly at a temperature of 70-80°C at a speed of 400-800r / min.
[0031] (2) Weigh 350g of water-based polyurethane emulsion and add it to step (1), and react for 20-40min while stirring in a water bath at 80-100°C.
[0032] (3) Weigh 4g of defoamer, 3g of preservative, and 7g of thickener and add them to step (2), and stir for 5 to 10 minutes at a speed of 400 to 800r / min; filter to obtain a water-based heat-insulating finish .
Embodiment 2
[0034] (1) Weigh 238g of glass microspheres, 250g of deionized water, 120g of filler and 70g of additives and stir evenly at a temperature of 70-80°C at a speed of 400-800r / min.
[0035] (2) Weigh 300g of water-based polyurethane emulsion and add it to step (1), and react for 20-40min while stirring in a water bath at 80-100°C.
[0036] (3) Weigh 5g of defoamer, 8g of preservative, and 9g of thickener and add them to step (2), and stir for 5 to 10 minutes at a speed of 400 to 800r / min; filter to obtain a water-based heat-insulating finish .
Embodiment 3
[0038] (1) Weigh 220g of glass microspheres, 242g of deionized water, 80g of filler and 50g of additives and stir evenly at a temperature of 70-80°C at a speed of 400-800r / min.
[0039] (2) Weigh 400g of water-based polyurethane emulsion and add it to step (1), and react for 20-40min while stirring in a water bath at 80-100°C.
[0040] (3) Weigh 2g of defoamer, 1g of preservative, and 5g of thickener and add them to step (2), and stir for 5-10 minutes at a speed of 400-800r / min; filter to obtain a water-based heat-insulating finish .
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com