Formula of finish material adopting travertinus dry powder
A facing material and formula technology, applied in the field of facing material formulation of dry powder Shihuanu, can solve the problems of increased decoration cost, unenvironmental protection, difficult storage, etc., and achieve the effects of long antifreeze shelf life, cost saving, and easy transportation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0010] The present invention will be further described below.
[0011] A kind of facing material formula of dry powder shihuanu of the present invention, it adopts following technical scheme:
[0012] Its raw material formula by weight percentage is as follows: 40%-60% of colored marble powder, 15%-25% of white cement, 10%-16% of calcite powder, 3%-8% of gray calcium, 1%-3% of attapulgite , Wood fiber 0.5%-3%, hydroxymethyl propyl cellulose 0.2%-0.8%, redispersible powder 0.8%-1.5%, water-soluble polyvinyl alcohol powder 0.2%-0.8%.
[0013] The raw material formula of the present invention by weight percentage is as follows: 50% of colored marble powder, 20% of white cement, 13% of calcite powder, 5% of lime calcium, 2% of attapulgite, 1.5% of wood fiber, 0.5% of hydroxymethyl propyl cellulose %, redispersible powder 1.25%, water-soluble polyvinyl alcohol powder 0.2%-0.8%.
[0014] Each raw material function among the present invention is as follows:
[0015] (1), colored m...