A diatomite asphalt mixture modifier and modified asphalt mixture

A technology of asphalt mixture and modifier, applied in building thermal insulation materials, building components, buildings, etc., can solve the problems of difficult quality control, easy brittle cracking, poor aging resistance, etc., so as to reduce production costs and improve quality. Stable, low cost effect

Inactive Publication Date: 2019-07-19
SICHUAN HONGHUI TECH
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] Ordinary road asphalt has poor temperature sensitivity, poor elasticity, and poor aging resistance without modification. It is prone to flow at high temperatures and brittle cracks at low temperatures. increase, the heavy load of vehicles increases, and the requirements for pavement materials continue to increase
[0003] The performance of asphalt pavement depends largely on the nature and quality of the asphalt mixture used. A lot of research has been done at home and abroad on the modification of asphalt and asphalt mixture. The currently studied modifiers include thermoplastic rubber. , such as SBS, SIS, SE / BS, etc.; Rubber, such as NR, SBR, CR, BR, etc.; Difficult to control quality, high energy consumption, poor environmental protection

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] (1) Clay-containing diatomite raw ore is crushed and hydraulically rotated and scrubbed, and then the obtained pulp solution is classified and refined by a cyclone at 0.2 MPa, and the obtained fineness is 325~400 mesh The diatomite slurry is subjected to 130kHz ultrasonic vibration for 5 minutes to obtain a refined soil slurry, and the refined soil slurry is press-filtered to obtain a refined soil filter cake with a water content of 40%, and then flashed to control its moisture content to less than 3.0%. Then drying to obtain activated diatomite;

[0028] (2) Mix activated diatomite with Tianshi 0330 type polyethylene wax to obtain the diatomite asphalt mixture modifier, wherein the mass ratio of polyethylene wax is 2%, and the polyethylene wax is synthetic polyethylene wax Wax resin, viscosity at 140°C is 200~400CPS;

[0029] (3) Conventionally mix the obtained diatomite asphalt mixture modifier with a mass of 1‰ of the asphalt mixture with the asphalt mixture to obta...

Embodiment 2

[0032] (1) Clay-containing diatomite raw ore is crushed and hydraulically rotated and scrubbed, and then the obtained pulp solution is classified and refined by a cyclone at 0.4MPa, and the obtained fineness is 500~600 mesh The diatomite slurry is subjected to 20kHz ultrasonic vibration for 15 minutes to obtain a refined soil slurry, and the refined soil slurry is press-filtered to obtain a refined soil filter cake with a water content of 50%, and then flashed to control its moisture content to less than 3.0%. Then drying to obtain activated diatomite;

[0033] (2) Mix activated diatomite with Tianshi 0330 type polyethylene wax to obtain the diatomite asphalt mixture modifier, wherein the mass ratio of polyethylene wax is 22%, and the polyethylene wax is a synthetic polyethylene wax Wax resin, viscosity at 140°C is 200~400CPS;

[0034] (3) Conventionally mix the obtained diatomite asphalt mixture modifier with a mass of 5‰ of the asphalt mixture with the asphalt mixture to ob...

Embodiment 3

[0037] (1) Clay-containing diatomite raw ore is crushed and hydraulically rotated and scrubbed, and then the obtained pulp solution is classified and refined by a cyclone at 0.3MPa, and the obtained fineness is 600~700 mesh The diatomite slurry is subjected to 100kHz ultrasonic vibration for 10 minutes to obtain a refined soil slurry, and the refined soil slurry is press-filtered to obtain a refined soil filter cake with a water content of 45%, and then flashed to control its moisture content to less than 3.0%. Then drying to obtain activated diatomite;

[0038] (2) In addition, polyethylene wax is prepared according to the mass ratio of polyethylene wax and activated diatomaceous earth as 20:80. The polyethylene wax is a synthetic polyethylene wax resin with a viscosity of 300~400CPS at 140°C;

[0039] (3) Add activated diatomite and polyethylene wax whose total mass is 3‰ of the asphalt mixture to the asphalt mixture for conventional mixing to obtain a modified asphalt mixtu...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a diatomite asphalt mixture modification agent and a modified asphalt mixture. The diatomite asphalt mixture modification agent is prepared from activated diatomite and polyethylene wax, wherein the mass percent of the polyethylene wax is 2%-22%; the activated diatomite is diatomite obtained by carrying out an activation step on diatomite raw ores; the activation step comprises the following steps of crushing the diatomite raw ores, scrubbing, grading and carrying out ultrasonic vibration; the fineness of the activated diatomite is 325-800 meshes. Compared with an asphalt mixture modified by SBS (Styrene Butadiene Styrene), the dynamic stability DS of the asphalt mixture modified by the modification agent is increased by at least 30%, the water stability (residue stability) is increased by at least 3% and the low-temperature anti-cracking performance (low-temperature failure strain) is improved by at least 1%.

Description

technical field [0001] The invention relates to the technical field of modifiers for asphalt mixtures. Background technique [0002] Ordinary road asphalt has poor temperature sensitivity, poor elasticity, and poor aging resistance without modification. It is prone to flow at high temperatures and brittle cracks at low temperatures. The increase in the number of vehicles and the increase in the heavy load of vehicles have increased the requirements for pavement materials. [0003] The performance of asphalt pavement depends largely on the nature and quality of the asphalt mixture used. A lot of research has been done at home and abroad on the modification of asphalt and asphalt mixture. The currently studied modifiers include thermoplastic rubber. , such as SBS, SIS, SE / BS, etc.; Rubber, such as NR, SBR, CR, BR, etc.; The quality is difficult to control, the energy consumption is high, and the environmental protection is poor. Contents of the invention [0004] The obje...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C08L95/00C08L23/06C08K9/00C08K3/34
CPCC08K3/346C08K9/00C08L95/00C08L2201/08C08L23/06
Inventor 刘天宝
Owner SICHUAN HONGHUI TECH
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products