LCD structure and manufacturing method thereof
A manufacturing method and color film technology, applied in nonlinear optics, instruments, optics, etc., can solve problems such as waste of manpower and man-hours, low output efficiency and yield, and large environmental pollution, so as to save material costs, reduce rework costs, The effect of reducing environmental pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] Example 1, such as figure 2 As shown, an LCD structure of the embodiment of the present invention includes an upper polarizer 1, an upper glass 2, a lower glass 3, a lower polarizer 4 and a color filter 5, and the bottom of the upper polarizer 1 is attached to the top of the upper glass 2 On, the bottom of the upper glass 2 is attached to the top of the lower glass 3 , the bottom of the lower glass 3 is attached to the top of the lower polarizer 4 , and the color filter 5 is attached to the bottom of the lower polarizer 4 .
[0037] Such as Figure 3-4 As shown, the color film 5 includes a release layer 501, a glue layer 502, a color layer 503 and a protective layer 504, the release layer 501 is attached to the top of the color layer 503 through the glue layer 502, and the bottom of the color layer 503 is attached with a protective layer 504 , the middle of the color layer 503 is a color area with a color pattern spray-painted.
[0038] Among them, the base material ...
Embodiment 2
[0039] Embodiment 2, a method for manufacturing an LCD structure described in the embodiment of the present invention, the method includes the following steps:
[0040] Step 1, attach the bottom of the upper glass 2 to the top of the lower glass 3 .
[0041] Step 2, attaching the bottom of the upper polarizer 1 to the top of the upper glass 2 , and attaching the lower polarizer 4 to the bottom of the lower glass 3 .
[0042] Step 3, make the color film 5 according to the requirement, including:
[0043] Step 301, confirm the pattern and color according to the requirements, and determine the thickness and external dimensions of the color filter 5;
[0044] Step 302, choose PET as the base material of the color film, make the base layer of the color layer 503, and spray-paint the required color and pattern on the base layer to obtain the color layer 503;
[0045] Step 303, attaching a protective layer 504 on the bottom of the colored layer 503;
[0046] Step 304 , attach the ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information